Simulated Hydrostatic Pulpal Pressure Effect on Microleakage—An Initial Study

MetadataDetails
Publication Date2024-04-18
JournalOperative Dentistry
AuthorsTD Wyatt, HW Roberts
InstitutionsUniversity of Kentucky

SUMMARY Purpose: This study’s purpose was to evaluate the effect of simulated in vitro hydrostatic pulpal pressure (HPP) on microleakage. Methods and Materials: Extracted third molars (n=12) were sectioned 5 mm below the cementoenamel junction, pulp tissue removed, and the sectioned crowns mounted on a Plexiglas plate penetrated by an 18-gauge stainless steel tube. The mounted specimen mesial surface received a 2×4×6 mm Class V preparation followed by restoration with a strongly acidic, one-step dental adhesive and a flowable microfilled resin, following all manufacturers’ instructions. Restorations were finished to contour, and tubing was attached to a 20-cm elevated, 0.2% rhodamine G reservoir to the specimen steel tube for 48 hours. Specimens then received a nail polish coating to within 1 mm of the restoration margins and were placed in 2% methylene blue (MB) dye for 24 hours, followed by rinsing, embedding in epoxy resin, and sectioning into 1 mm slices using a diamond saw. Controls were intact molars (n=12) processed as above but without HPP. Specimen slices were evaluated using laser confocal microscopy with images exported to ImageJ software with microleakage assessed as the MB linear penetration as a percentage of the total interfacial wall length. Mean values were evaluated with the Kruskal Wallis/Dunn test at a 95% confidence level. Results: The control specimens demonstrated significantly greater (p<0.0001) MB penetration than experimental specimens with simulated HPP. Under this study’s conditions, simulated HPP significantly decreased MB dye penetration. Conclusion: Studies accomplished without simulated HPP may overestimate microleakage results.

  1. 2009 - Membrane permeability properties of dental adhesive films
  2. 2020 - Marginal integrity of flowable and packable bulk fill materials used for class II restorations -A systematic review and meta-analysis of in vitro studies
  3. 1976 - Microleakage: A review
  4. 1997 - Detection of microleakage around dental restorations: A review
  5. 2017 - Review of microleakage evaluation tools
  6. 2002 - Can modern restorative procedures and materials reliably seal cavities? In vitro investigations, Part 1
  7. 2002 - Can modern restorative procedures and materials reliably seal cavities? In vitro investigations, Part 2
  8. 2001 - Association between microtensile bond strength and leakage in the indirect resin composite/dentin adhesively bonded joint
  9. 2001 - Relationship between bond strengths and nanoleakage: Evaluation of a new assessment method
  10. 2005 - Class II composite resin restorations with two polymerization techniques: Relationship between microtensile bond strength and marginal leakage