Abstract
Section titled “Abstract”In this work, first, we investigate the effect of nitrogen addition in microwave plasma enhanced chemical vapor deposition on the growth of thick {113} epitaxial diamond layers. We identify a narrow range of nitrogen concentrations for the growth of crack-free thick epitaxial layers with a smooth surface morphology. Without nitrogen, cracks start to appear after a layer thickness of 7-10 μm due to elastic energy stored in the epitaxial layer, but the addition of nitrogen stabilizes layer growth. We also investigate the use of low microwave power density growth conditions to produce thick boron-doped epitaxial layers. We observe a very high boron incorporation efficiency using these growth conditions. Finally, we demonstrate the fabrication of a thick (>200 μm) {113} p+ monocrystal plate. The concentration of boron in heavily doped diamond with metallic conductivity has been investigated by the Hall effect measurement technique, Raman spectroscopy, and secondary ion mass spectroscopy. The growth of high quality thick {113} oriented epitaxial layer with high boron concentration (>1020 cm−3) and low resistivity and the fabrication for the freestanding p+ substrates are necessary steps for the fabrication of vertical electronic devices such as high power Schottky diodes.
Tech Support
Section titled “Tech Support”Original Source
Section titled “Original Source”References
Section titled “References”- 2014 - Zr/oxidized diamond interface for high power Schottky diodes [Crossref]
- 2013 - Sensing of phosgene by a porous-like nanocrystalline diamond layer with buried metallic electrodes [Crossref]
- 2012 - High temperature application of diamond power device [Crossref]
- 2016 - Electrical properties of diamond platinum vertical Schottky barrier diodes [Crossref]
- 2021 - Heteroepitaxy growth of single crystal diamond on Ir/Pd/Al2O3 (11-20) substrate [Crossref]
- 2004 - Single crystal diamond for electronic applications [Crossref]
- 2009 - CVD Diamond for Electronic Devices and Sensors
- 2019 - Thick and widened high quality heavily boron doped diamond single crystals synthetized with high oxygen flow under high microwave power regime [Crossref]
- 2017 - Thick heavily boron doped CVD diamond films homoepitaxially grown on (111)-oriented substrates [Crossref]
- 2016 - Growth of thick and heavily boron-doped (113)-oriented CVD diamond films [Crossref]