Abstract
Section titled āAbstractāAll-dielectric metasurfaces offer a low-loss alternative to plasmonic metasurfaces. We proposed the configuration for high-reflectivity all-dielectric metasurfaces based on single-crystal diamond (SCD) resonators on fused silica substrate and conducted simulations to optimize and analyze such a configuration via the FDTD solver. We utilized GMR as the design principle to select the configuration and the substrate material, and analyzed the scattering properties of a single SCD resonator by multipole decomposition. Then, we demonstrated that both the cylindrical resonators in square lattice and frustum-shaped resonators in hexagonal lattice can achieve near-unity reflectivity (>99.99%) and ultra-low absorption (<0.001%) at 795 nm, the typical alkali-metal laser wavelength. Additionally, we demonstrated that such a design is quite tolerant of fabrication errors and further supports its potential for realistic applications. To expand the functionality of such devices across multiple wavelengths, dual-band high-reflectivity metasurfaces at 744 nm and 828 nm were also designed. Our work is quite useful for designing diamond-based highly reflective mirrors, paving the way for low-loss all-dielectric reflective metasurfaces in high-power laser applications.
Tech Support
Section titled āTech SupportāOriginal Source
Section titled āOriginal SourceāReferences
Section titled āReferencesā- 2012 - From Metamaterials to Metadevices [Crossref]
- 2011 - Metamaterials: A New Frontier of Science and Technology [Crossref]
- 2020 - Flat Optics with Dispersion-Engineered Metasurfaces [Crossref]
- 2016 - A Review of Metasurfaces: Physics and Applications [Crossref]
- 2023 - Recent Advanced Applications of Metasurfaces in Multi-dimensions [Crossref]
- 2023 - Real Time Full-color Imaging in a Meta-optical Fiber Endoscope [Crossref]
- 2020 - Complex-Amplitude Metasurface-Based Orbital Angular Momentum Holography in Momentum Space [Crossref]
- 2017 - Arbitrary Spin-to-Orbital Angular Momentum Conversion of Light [Crossref]
- 2023 - Folded Digital Meta-Lenses for On-Chip Spectrometer [Crossref]
- 2020 - Metasurface for Structured Light Projection over 120° Field of View [Crossref]