Advanced 3D-Printed Flexible Composite Electrodes of Diamond, Carbon Nanotubes, and Thermoplastic Polyurethane
At a Glance
Section titled āAt a Glanceā| Metadata | Details |
|---|---|
| Publication Date | 2024-11-19 |
| Journal | ACS Applied Polymer Materials |
| Authors | Simona BaluchovÔ, Stach van Leeuwen, BarıŠKumru, Josephus G. Buijnsters |
| Institutions | Charles University, Delft University of Technology |
| Citations | 6 |
Abstract
Section titled āAbstractāIn this work, we pioneered the preparation of diamond-containing flexible electrodes using 3D printing technology. The herein developed procedure involves a unique integration of boron-doped diamond (BDD) microparticles and multi-walled carbon nanotubes (CNTs) within a flexible polymer, thermoplastic polyurethane (TPU). Initially, the process for the preparation of homogeneous filaments with optimal printability was addressed, leading to the development of two TPU/CNT/BDD composite electrodes with different CNT:BDD weight ratios (1:1 and 1:2), which were benchmarked against a TPU/CNT electrode. Scanning electron microscopy revealed a uniform distribution of conductive fillers within the composite materials with no signs of clustering or aggregation. Notably, increasing the proportion of BDD particles led to a 10-fold improvement in conductivity, from 0.12 S m<sup>-1</sup> for TPU/CNT to 1.2 S m<sup>-1</sup> for TPU/CNT/BDD (1:2). Cyclic voltammetry of the inorganic redox markers, [Ru(NH<sub>3</sub>)<sub>6</sub>]<sup>3+/2+</sup> and [Fe(CN)<sub>6</sub>]<sup>3-/4-</sup>, also revealed a reduction in peak-to-peak separation (Ī<i>E</i> <sub>p</sub>) with a higher BDD content, indicating enhanced electron transfer kinetics. This was further confirmed by the highest apparent heterogeneous electron transfer rate constants (<i>k</i> <sup>0</sup> <sub>app</sub>) of 1 Ć 10<sup>-3</sup> cm s<sup>-1</sup> obtained for both markers for the TPU/CNT/BDD (1:2) electrode. Additionally, the functionality of the flexible TPU/CNT/BDD electrodes was successfully validated by the electrochemical detection of dopamine, a complex organic molecule, at millimolar concentrations by using differential pulse voltammetry. This proof-of-concept may accelerate development of highly desirable diamond-based flexible devices with customizable geometries and dimensions and pave the way for various applications where flexibility is mandated, such as neuroscience, biomedical fields, health, and food monitoring.