MnO2-Conductive Nanodiamond Composite Electrode for High Energy Density Aqueous Capacitor
At a Glance
Section titled âAt a Glanceâ| Metadata | Details |
|---|---|
| Publication Date | 2024-11-22 |
| Journal | ECS Meeting Abstracts |
| Authors | Masafumi Imai, Takeshi Kondo |
Abstract
Section titled âAbstractâElectric double-layer capacitors (EDLC) have the advantage of faster charge-discharge rates and superior cycle life compared to rechargeable batteries, but have the disadvantage of low energy density. In order to increase energy density of EDLCs, it is necessary to increase cell voltage and specific surface area. Another possible strategy to enhance the energy density is combination with redox-active compounds to form pseudocapacitor. We have developed boron-doped nanodiamond (BDND) as a novel electrode material for EDLC, which has a wide potential window in aqueous electrolytes, high voltage application capability, and large specific surface area. The aim of this study is to fabricate a pseudocapacitor by compositing BDND with MnO 2 in order to further improve the energy density. BDND was prepared by depositing a boron-doped diamond (BDD) layer on the surface of nanodiamond particles by microwave plasma CVD followed by heat treatment in air to minimize the sp 2 carbon impurities. BDND ink was prepared by mixing BDND and ethanol. The BDND ink was then applied on a glassy carbon current collector, and MnO 2 -BDND electrodes were prepared by electrodeposition of MnO 2 on the BDND using constant potential electrolysis in 0.6 M MnSO 4 /0.8 M H 2 SO 4 at +1.25 V vs. Ag/AgCl. Cyclic voltammetry (CV) in 1 M Na 2 SO 4 was used to evaluate the electrochemical properties of the MnO 2 -BDND electrode. MnO 2 -BDND electrodes were prepared with various MnO 2 deposition times of 1, 3, 5, and 15 min. It was found from the CV current density that the MnO 2 -BDND prepared at a deposition time of 3 min exhibited the largest capacitance of 43.5 F/g, while the capacitance of unmodified BDND electrode was 14.5 F/g. Therefore, MnO 2 deposition time of 3 min was determined to be the optimum condition; the reason for the decrease in the CV current of MnO 2 -BDND with a deposition time of 5 and 15 min is considered to be due to excess amount of MnO 2 with poor conductivity on the electrode surface. Energy density of the MnO 2 -BDND/1 M Na 2 SO 4 system was calculated with a cell voltage of 1.5 V to be 21.2 Wh/kg, which was greater than that of the BDND/1 M Na 2 SO 4 system (9.1 Wh/kg). Therefore, BDND-based high energy density aqueous capacitor is expected to be fabricated by the combination with MnO 2 .