Controlling electrochemical lignin depolymerization via halide chemistry at boron-doped diamond electrodes

MetadataDetails
Publication Date2025-01-01
JournalRSC Advances
AuthorsBusarakham Ngokpho, Pattarawadee Therdkatanyuphong, Panot Krukkratoke, Tanatorn Khotavivattana, Apichat Boontawan
InstitutionsChulalongkorn University, Suranaree University of Technology

Green electrochemical method for lignin depolymerization, tunable via halide mediation at boron-doped diamond electrodes.