Skip to content

Flexible thermal interface materials based on diamond–graphene composite films prepared at different temperatures

MetadataDetails
Publication Date2025-03-01
JournalApplied Physics Letters
AuthorsYifan Xu, Huiqiang Liu, Bing Wang, Wen Zhang, Zhaoxin Zhong
InstitutionsUniversity of Electronic Science and Technology of China, Southwest University of Science and Technology
Citations1

Diamond and graphene, which have extremely high thermal conductivity, are considered ideal candidates for the preparation of high-performance thermal interface materials (TIMs). However, the development of flexible TIMs with efficient heat transfer paths still hampers their thermal management applications. Herein, a highly oriented diamond-graphene composite film (DGCF) was prepared by one-step microwave plasma chemical vapor deposition on carbon cloth (CC) using N-butylamine as a single liquid carbon source. The hybridized composition of sp3/sp2 and the heat transfer path length of DGCF are regulated by the deposition temperature and the thermal conductivity of CC/DGCF at 30 °C is 2.71 W m−1 K−1, which is 15 times higher than that of CC. Further flexible TIMs of CC/DGCF are achieved using thermal silicone grease (TG) as filler, and the thermal conductivity of the final flexible compound of CC/DGCF/TG is 6.97 W m−1 K−1 at 30 °C, which is 39 times higher than that of pure CC and 2 times higher than that of TG, respectively. In the actual TIMs performance test, the cooling efficiency is 1.4 times higher than that of the commercial thermal conductive silicone pad. Furthermore, finite element simulations demonstrated that the film at 800 °C has the optimal sp3/sp2 ratio for thermal response and the best thermal conductivity path structure. This finding provides a method for the design of highly flexible TIMs and increases the possibility of their practical application in electronic thermal management.

  1. 2024 - Comprehensive review and future prospects on chip-scale thermal management: Core of data center’s thermal management [Crossref]
  2. 2024 - Advancements and challenges in thermoregulating textiles: Smart clothing for enhanced personal thermal management [Crossref]
  3. 2024 - Carbon-based materials with combined functions of thermal management and electromagnetic protection: Preparation, mechanisms, properties, and applications [Crossref]
  4. 2015 - Thermal properties of graphene and few-layer graphene: Applications in electronics [Crossref]
  5. 2024 - Review on phase change materials for spacecraft avionics thermal management [Crossref]
  6. 2024 - 3D carbon based phase change composites: A review on progress in fabrication strategies, thermal energy storage conversion efficacy, prototypes, numerical models and applications [Crossref]
  7. 2012 - Thermal properties of the hybrid graphene-metal nano-micro-composites: Applications in thermal interface materials [Crossref]
  8. 2024 - 2D materials-based thermal interface materials: Structure, properties, and applications [Crossref]
  9. 2016 - Thermal and mechanical properties of carbon fiber polymer-matrix composites with a 3d thermal conductive pathway [Crossref]
  10. 2017 - MgO nanoparticles-decorated carbon fibers hybrid for improving thermal conductive and electrical insulating properties of Nylon 6 composite [Crossref]