Enhanced channel mobility of hexagonal boron nitride/hydrogen-terminated diamond heterojunction field-effect transistor
At a Glance
Section titled āAt a Glanceā| Metadata | Details |
|---|---|
| Publication Date | 2025-10-06 |
| Journal | Applied Physics Letters |
| Authors | Yosuke Sasama, Takuya Iwasaki, Masataka Imura, Kenji Watanabe, Takashi Taniguchi |
| Institutions | National Institute for Materials Science, University of Tsukuba |
Abstract
Section titled āAbstractāHydrogen-terminated diamond field-effect transistors (FETs) using a hexagonal boron nitride (h-BN) gate insulator were fabricated on a diamond surface with reduced surface roughness in the direction of source/drain electrodes. The diamond surface was prepared on a mesa structure using chemical vapor deposition with a low methane concentration. The hydrogen-terminated surface was laminated with the h-BN gate insulator without air exposure to prevent the adsorption of atmospheric surface acceptors. The hydrogen-terminated diamond FET exhibited a high mobility of ā1000 cm2 Vā1 sā1 at room temperature. We performed theoretical analysis on the temperature and carrier density dependences of mobility, which suggested that Coulomb and surface roughness scattering were effectively reduced. The high mobility obtained in this study indicates the high potential of diamond as a semiconducting material. This study can contribute to the future development of diamond devices.
Tech Support
Section titled āTech SupportāOriginal Source
Section titled āOriginal SourceāReferences
Section titled āReferencesā- 2020 - Diamond power devices: State of the art, modelling, figures of merit and future perspective [Crossref]
- 2024 - Diamonds in the current: Navigating challenges for the integration of diamond in power electronics [Crossref]
- 1994 - Enhancement mode metal-semiconductor field effect transistors using homoepitaxial diamonds [Crossref]
- 2012 - Diamond junction field-effect transistors with selectively grown n+-side gates [Crossref]
- 2017 - Deep-depletion mode boron-doped monocrystalline diamond metal oxide semiconductor field effect transistor [Crossref]
- 1996 - Hydrogen-terminated diamond surfaces and interfaces [Crossref]
- 2006 - Structure, electronics, and interaction of hydrogen and oxygen on diamond surfaces [Crossref]
- 2023 - Diamond p-FETs using two-dimensional hole gas for high frequency and high voltage complementary circuits [Crossref]
- 2000 - Origin of surface conductivity in diamond [Crossref]
- 2017 - Diamond field-effect transistors for RF power electronics: Novel NO2 hole doping and low-temperature deposited Al2O3 passivation [Crossref]