Field-effect detected magnetic resonance of nitrogen-vacancy centers in diamond based on all-carbon Schottky contacts
At a Glance
Section titled “At a Glance”| Metadata | Details |
|---|---|
| Publication Date | 2025-12-02 |
| Journal | Communications Engineering |
| Authors | Xuan Phuc Le, Ludovic Mayer, Simone Magaletti, Martin U. Schmidt, Jean-François Roch |
| Institutions | Centre National de la Recherche Scientifique, Thales (Australia) |
| Analysis | Full AI Review Included |
Technical Documentation: All-Carbon Schottky Contacts for NV Center Magnetic Resonance Detection
Section titled “Technical Documentation: All-Carbon Schottky Contacts for NV Center Magnetic Resonance Detection”Executive Summary
Section titled “Executive Summary”- Breakthrough Approach: The paper demonstrates a novel all-carbon graphitic-diamond-graphitic device functioning as two back-to-back Schottky diodes, enabling purely electrical readout of Nitrogen-Vacancy (NV) center spin resonances without conventional ohmic contacts.
- Material Insight: Under 561 nm illumination, the NV center ensemble generates electron-hole pairs that transform a lightly doped type IIa diamond (1 ppm N, ~50 ppb B) into a p-type semiconductor, enabling localized Schottky barrier formation at graphitic electrodes.
- Physical Mechanism: Spin-dependent thermionic emission across the reverse-biased Schottky junction produces a photocurrent modulated by RF-driven NV− spin transitions, with a measured zero-field splitting (ZFS) of 2.87 GHz.
- Contrast Performance: Photoelectric Detection of Magnetic Resonance (PDMR) contrast reaches up to ~18% under optimal conditions, with electric contrast exceeding optical contrast via a field-effect mechanism tied to depletion region (DR) modulation.
- Electrode Fabrication: Graphitic electrodes of 50 × 50 µm2 (200 µm gap) are created via Xenon Focused Ion Beam (FIB) implantation at a dose of 4×1015 cm−2 (30 keV), yielding optically semi-transparent contacts (~70% transmission).
- Quantum Sensing Application: Establishes a pathway for miniaturized NV-based magnetometry, electrometry, thermometry, and RF sensing with simplified wiring (e.g., parallel-plate architectures).
Technical Specifications
Section titled “Technical Specifications”| Parameter | Value | Unit | Context |
|---|---|---|---|
| Diamond Material Grade | Type IIa (Optical Grade) | — | Element Six (E6) CVD-grown single crystal |
| Nitrogen Concentration | 1 | ppm | Dominant dopant |
| NV Center Concentration | Few | ppb | Creation yield ~0.3% |
| Boron Concentration | ~50 | ppb | Parasitic CVD doping |
| Crystal Orientation | ⟨100⟩ / ⟨110⟩ side facets | — | Optically polished side facets |
| Laser Wavelength (Pumping) | 561 | nm | CW green excitation (Cobolt Jive) |
| NV− Zero-Field Splitting (D) | 2.87 | GHz | Ground state triplet splitting |
| Gyromagnetic Ratio (γe) | 28 | GHz/T | For magnetic field Zeeman shift |
| ZPL NV0 | 575 | nm | Neutral charge state |
| ZPL NV− | 637 | nm | Negative charge state |
| Electrode Dimensions | 50 × 50 | µm2 | Graphitic contacts |
| Inter-Electrode Gap | 200 | µm | Lateral separation |
| Electrode Thickness | Few | nm | Xenon FIB-induced graphitization |
| Electrode Optical Transmission | ~70 | % | Allows simultaneous ODMR imaging |
| Xenon Implantation Dose | 4×1015 | cm−2 | Ion beam parameter |
| Xenon Implantation Energy | 30 | keV | Ion beam parameter |
| Applied Bias Voltage Range | 0 to ±300 | V | DC bias across structure |
| Laser Power Range | 65 to 400 | mW | At laser output |
| Beam Waist Range (w0) | 6.4 to 11.9 | µm | At electrode area |
| Pump Intensity (Active Area) | ~100 | kW/cm2 | 65 mW with 6.4 µm waist |
| RF Power | 25 | dBm | Driving NV− spin transitions |
| Transition Voltage (400 mW, 11.9 µm) | ~100 | V | DR reaches illumination depth limit |
| Field Gradient Resonance (Electrode A) | 1.98 | GHz | NV− ∣0⟩→∣±1⟩ transition |
| Field Gradient Resonance (Electrode B) | 2.02 | GHz | NV− ∣0⟩→∣±1⟩ transition |
| Simulated Hole Density (p0) | 1.28×1014 | cm−3 | Under laser illumination |
| Conductive Channel Depth (D) | 16.8 | µm | Gaussian beam penetration depth |
| PDMR Maximum Contrast | ~18 | % | Best at 400 mW, 100-125 V bias |
| ODMR/PDMR Measurement Time | ~6 / ~9 | min | For 250 frequency points |
| Diamond Band Gap | 5.5 | eV | Reference parameter |
Key Methodologies
Section titled “Key Methodologies”- Diamond Sample Preparation: Use a ⟨100⟩-oriented type IIa optical grade CVD single crystal diamond with 1 ppm nitrogen and ~50 ppb boron; polish side facets to optical quality without post-growth irradiation or annealing.
- Graphitic Electrode Fabrication: Create 50 × 50 µm2 graphitic electrodes separated by 200 µm via Xenon Focused Ion Beam (FIB) implantation at a dose of 4×1015 cm−2 and energy of 30 keV to convert a surface diamond layer into amorphous/graphitic carbon.
- Optical Pumping: Apply continuous-wave (CW) green laser excitation at 561 nm through a 5 cm lens focused on the side facet of the diamond, creating an optical path between the two electrodes.
- Beam Profiling: Adjust the beam waist (w0) between 6.4 µm and 11.9 µm using an afocal doublet to tune the conductive channel depth beneath the electrodes.
- Electrical Readout Setup: Apply a DC bias voltage from a high-voltage Source Measure Unit (SMU, Keithley 2470) ranging from 0 to ±300 V across the graphitic contacts and monitor photocurrent.
- RF Excitation: Drive NV− spin transitions using a loop antenna centered over the electrodes at the zero-field resonance frequency of 2.87 GHz with 25 dBm RF power.
- Magnetic Field Mapping: Apply a static magnetic field with a gradient along one ⟨111⟩ diamond axis via a neodymium permanent magnet to spatially separate the four NV center families by resonance frequency (1.98 GHz at A, 2.02 GHz at B).
- Optical Readout: Collect photoluminescence through a Mitutoyo M Plan Apo 10× objective (NA 0.28) with NV0 (584/40 nm) or NV− (698/70 nm) bandpass filters onto a CMOS camera.
- Depletion Region Visualization: Acquire ΔPL images by subtracting PL frames at applied bias (e.g., +150 V) from frames at 0 V bias using NV− and NV0 filters to image band bending effects.
- COMSOL Multiphysics Simulation: Model the electric field profile and DR extension as a function of bias voltage assuming a homogeneous hole density of 1.28×1014 cm−3 over a 16.8 µm depth.
6CCVD Solutions & Capabilities
Section titled “6CCVD Solutions & Capabilities”Applicable Materials
Section titled “Applicable Materials”- Optical Grade SCD (Single Crystal Diamond): The research uses a type IIa ⟨100⟩ optical grade single crystal diamond with controlled nitrogen (~1 ppm) and trace boron (~50 ppb) doping. 6CCVD supplies high-purity optical grade SCD substrates with precisely tuned nitrogen content suitable for NV ensemble magnetometry.
- Boron-Doped (BDD) Substrates: For researchers seeking to enhance the p-type conductivity or modify the boron-to-nitrogen compensation ratio, 6CCVD offers custom boron-doped SCD and PCD with controllable dopant concentrations.
- Polycrystalline Diamond (PCD) Wafers: For scalable, cost-effective production of NV sensor arrays, 6CCVD’s inch-size PCD wafers (polished to Ra < 5 nm) provide an alternative geometry suitable for large-area Schottky device arrays.
Customization Potential
Section titled “Customization Potential”- Custom Crystallographic Orientation: 6CCVD provides ⟨100⟩, ⟨110⟩, and ⟨111⟩-oriented SCD substrates with optical-grade side-facet polishing capabilities for lateral illumination schemes like the one demonstrated.
- Laser Cutting & Micro-Fabrication: 6CCVD offers laser cutting and shaping services to produce non-standard geometries, micro-channels, and tailored side-facet surfaces required for side-pumped NV sensing devices.
- Doping Engineering: Custom nitrogen and boron doping profiles during MPCVD growth can be specified to achieve the precise NV-center yield (~0.3% demonstrated) and charge compensation dynamics required for Schottky-based readout.
- Surface Preparation: Polishing capabilities include Ra < 1 nm for SCD surfaces, enabling high-quality graphitic electrode formation via ion implantation or alternative metallization schemes.
Engineering Support
Section titled “Engineering Support”- 6CCVD’s in-house PhD engineering team provides consultation on material selection for NV-center quantum sensing projects, including magnetometry, electrometry, thermometry, and RF sensing applications.
- Technical guidance is available for replicating the Schottky-contact device architecture, including recommendations on crystal orientation, doping profiles, and thickness selection (SCD/PCD thickness range: 0.1 µm to 500 µm; substrates up to 10 mm).
- Metallization Support: For variants of this all-carbon device requiring hybrid metal contacts, 6CCVD provides in-house metalization with Au, Pt, Pd, Ti, W, and Cu to fabricate Schottky or ohmic electrodes tailored to specific barrier heights.
Call to Action
Section titled “Call to Action”For custom specifications, tailored doping concentrations, or material consultation for NV-center quantum sensor projects, visit 6ccvd.com or contact our engineering team directly.
View Original Abstract
The nitrogen-vacancy (NV) center is a defect in diamond whose spin state can be read optically by exploiting its photoluminescence or electrically by exploiting its charge generation rate under illumination, both of which being spin-dependent. The latter method offers numerous opportunities in terms of integration and performance compared to conventional optical readout. Here, we investigate the physical properties of a graphitic-diamond-graphitic structure under illumination. We show how, for a type IIa diamond material, electron-hole pairs generated by an ensemble of NV centers lead to a p-type material upon illumination, making this all-carbon structure equivalent to two back-to-back Schottky diodes. We analyze how the reverse current flowing upon illumination changes as a function of bias voltage and radiofrequency-induced excitation of the NV ensemble spin resonances. Furthermore, we demonstrate how an additional field effect arising from the illumination scheme affects the reverse current, resulting in a photoelectrical signal that can exceed the optical signal under the same illumination conditions. Xuan Phuc Le and colleagues report on the photoelectric detection of spin resonances in nitrogen-vacancy centres in a graphitic-diamond-graphitic structure. Behaving like two back-to-back Schottky diodes, it produces an enhanced photoelectric signal.