Field plate multi-finger diamond MOSFET with ampere-class current capability and a breakdown voltage of 550 V
Paper details
Section titled “Paper details”| Field | Value |
|---|---|
| Journal | Applied Physics Express |
| Published | 2026-02-24 |
| Authors | Sadao Shoji, Nobutaka Oi, Sora Kawai, Ryo Yoshida, Kosuke Ota |
| DOI | 10.35848/1882-0786/ae49df |
| Citations | 2 |
A gate field plate enabled a 5.4 mm-wide multi-finger diamond MOSFET to reach a 550 V breakdown voltage while delivering 0.82 A. The device also switched 1.0 A at a -200 V supply, with a 56 ns rise time and a 15 ns fall time. This was the first reported diamond MOSFET to combine ampere-class current with a breakdown voltage above 500 V. The authors attribute the improved blocking behavior to lower electric field concentration at the gate metal.
Field plate design target
Section titled “Field plate design target”Power MOSFETs need high current, high blocking voltage, and low off-state leakage. Earlier diamond devices did not combine all three at high current.
The gate field plate, or GFP, sits on the Al2O3 insulator at the same potential as the gate. Its purpose is to relax the electric field at the gate edge.
Diamond’s 5.47 eV bandgap and 22 W (cm·K)−1 thermal conductivity were cited as advantages for power electronics. Hydrogen-terminated diamond supplied the two-dimensional hole gas used as the channel.
Device construction and process
Section titled “Device construction and process”The base was a (001)-oriented crystalline diamond substrate. MPCVD added a buffer layer and a 200 nm unintentionally doped layer. Heavily boron-doped source and drain contact layers were grown selectively using a SiO2 hard mask.
Hydrogen plasma formed the channel termination. Remote O2 plasma produced oxygen-terminated isolation outside the protected active area.
A 200 nm Al2O3 gate insulator was deposited by high-temperature ALD at 723 K with H2O as oxidant. Tetramethylammonium hydroxide selectively wet etched the 200 nm Al2O3. Electron-beam evaporation deposited 200 nm Al, and lift-off formed the gate electrode. PECVD added SiO2 passivation at 623 K.
The GFP and drain contact used a sputtered 30/300 nm Ti/Al stack. The source metal and large pads used 30/1000 nm Ti/Al. Photolithography and ICP-RIE defined the metal patterns and contact openings. A final 1 μm SiO2 film passivated the surface before source opening.
Static characteristics were measured with a Keysight B1505 at 298 K under vacuum. The multi-finger die was bonded to direct-bonded copper and wire bonded for switching tests.
Devices A through C were single-finger devices. Device D was multi-finger. Devices A and B had 4 μm source-gate spacing, a 3 μm gate length, and a 10 μm gate-drain spacing. Device C used a 12 μm gate-drain spacing. Device D used 5 μm source-gate spacing, a 3 μm gate length, and a 10 μm gate-drain spacing.
Device A had no GFP. Device B used a 4 μm GFP, Device C a 6 μm GFP, and Device D a 6 μm GFP. Gate widths were 0.07 mm for A, B and C, and 5.4 mm for D.
Single-finger field plate results
Section titled “Single-finger field plate results”Breakdown was defined as the VDS at which drain current density reached 0.1 μA mm−1. Device A had no field plate and broke down at -290 V with VGS at 45 V.
Device B used a 4 μm field plate and reached -660 V at the same VGS. Device C used a 6 μm field plate and reached -845 V with VGS at 47 V. The field-plate devices therefore broke down at more than twice the voltage of Device A.
Off-state leakage and gate leakage were also much lower than for Device A. Similar transfer curves showed that the GFP preserved current capability while raising breakdown voltage. All single-finger devices had an on/off ratio above eight orders of magnitude.
Multi-finger output and blocking
Section titled “Multi-finger output and blocking”The multi-finger device broke down at VDS of -550 V with VGS at 52 V. Its 5.4 mm total gate width supported 0.82 A.
At VDS = -40 V and VGS = -20 V, the maximum drain current was 0.82 A. The corresponding drain current density was 152.8 mA mm−1 and the specific on-resistance was 261.8 Ω·mm.
At VGS = 42 V, drain current remained at the lower measurement limit. The on/off ratio exceeded nine orders of magnitude.
The 550 V breakdown was the highest reported for an ampere-class diamond MOSFET. Its magnitude was lower than the 660 V and 845 V field-plate single-finger results.
The authors attribute the reduction to lithography and etching variations in the gate or GFP metal shape. Those shape differences produced variation among devices in the multi-finger structure.
Switching under high voltage
Section titled “Switching under high voltage”Double-pulse tests covered VDD of -100 V and -200 V. The gate was driven at 40 V and -10 V.
At VDD = -100 V and a drain current of 0.2 A, rise time was 16 ns and fall time was 41 ns. At VDD = -200 V and a drain current of 1.0 A, rise time was 56 ns and fall time was 15 ns.
The authors define rise time as the VDS drop from 90% to 10%. Fall time is the VDS rise from 10% to 90%.
The switching device was mounted on direct-bonded copper with wire bonds. Active area, gate drive, test conditions, and parasitic capacitance affect timing. The measurements show fast switching with ampere-class current and 200-V-class supply.
Comparison with prior diamond MOSFETs
Section titled “Comparison with prior diamond MOSFETs”Kitabayashi et al. reported 2 kV breakdown, but the on-state current density was low, at 1 to 10 mA mm−1. Those measurements used VDS of -50 V and VGS of -30 V.
Saha et al. reported breakdown voltages of 2.6 to 4.3 kV, with off-state leakage of 0.1 to 10 mA mm−1. This work reaches a lower breakdown voltage than those high-voltage devices. Its result combines 550 V blocking with 0.82 A output and low measured off-state drain current.
The paper therefore identifies this device as the first diamond MOSFET to demonstrate both high breakdown voltage and ampere-class current. The current work differs by demonstrating switching at 200 V with ampere-class current.
The reported switching conditions were:
| Study | Voltage condition | Drain current | Rise time | Fall time |
|---|---|---|---|---|
| Saha et al. | -105 V | 0.015 A | 6.73 ns | 4.09 ns |
| Takaesu et al. | -30 V | 2.5 A | 19 ns | 32 ns |
| This work, lower-voltage case | -100 V | 0.2 A | 16 ns | 41 ns |
| This work, high-voltage case | -200 V | 1.0 A | 56 ns | 15 ns |
These times are not directly comparable because the studies used different gate-drive circuits, test conditions, and active areas. Parasitic capacitance also differed with active area.
Limits for power-device engineering
Section titled “Limits for power-device engineering”The main unresolved issue is electric field concentration at the gate or GFP edge. Drain and gate leakage were similar near breakdown, which supports this diagnosis. The authors expect further optimization of the field relaxation structure to improve breakdown voltage.
Field-plate geometry cannot be separated completely from other design changes in Devices B and C. Their field-plate lengths and gate-drain spacings differ, as do their gate voltages. Device A versus B provides the cleaner field-plate comparison. Both had a 10 μm gate-drain spacing and were tested at VGS of 45 V.
Multi-finger fabrication also needs tighter control of lithography and etching. Shape variation reduced breakdown from the best single-finger result to -550 V.
Static data were obtained at 298 K under vacuum. No long-term stability test or reliability qualification is reported in the paper. The demonstrated operating point is VDS of -40 V, VGS of -20 V, and a drain current of 0.82 A.
Materials and support
Section titled “Materials and support”The MOSFET requires a (001)-oriented crystalline diamond substrate with a 200 nm MPCVD UID layer and selectively boron-doped source and drain contacts. The 6CCVD diamond materials catalog lists MPCVD single-crystal and polycrystalline diamond, boron-doped material, and single-crystal thicknesses from 0.1 to 500 μm.
Plates and wafers up to 125 mm and Ti metallization can be checked against the paper’s substrate and Ti/Al stacks through the engineering support page.
View Original Abstract
Abstract The field plate structure is an effective technique for improving breakdown characteristics. In this work, the gate field plate (GFP) diamond MOSFET with both ampere-class current capability and high breakdown voltage is demonstrated for the first time. The maximum drain current of the fabricated device was 0.82 A with a breakdown voltage of 550 V. From the double pulse test, the rise time and fall time are 56 ns and 15 ns, respectively, even at a supply voltage of −200 V and a drain current of 1 A. These results indicate that a diamond MOSFET is promising for power devices.
Boron Doped Single Crystal Diamond Plate
View Specs →
Boron Doped Diamond On Titanium Bdd Electrode
View Specs →