Advanced Electro-Thermal Modeling of Edge Termination in Diamond and Ultra-Wide Bandgap Power Devices
Paper details
Section titled “Paper details”| Field | Value |
|---|---|
| Journal | IEEE Transactions on Electron Devices |
| Published | 2026-03-18 |
| Authors | Martin Kah, Nazareno Donato, Nicolas Rouger, Rebecca J. Watkins, Calum S. Henderson |
| DOI | 10.1109/ted.2026.3669152 |
The hybrid phosphorus-doped JTE and Al2O3 field plate showed the greatest simulated likelihood of withstanding a 1200 V reverse transient. At 10 ms after reaching 1100 V, the simulation reported a 30% reduction in peak field for the hybrid termination. The diamond surface field fell by up to 90% in the same comparison. Both field values came from a 10^6 V/s ramp. Quasi-static modeling had ranked the JTE-only design more favorably, so the transient result favors a different termination for fast-switching diamond devices.
Transient stress changes the termination ranking
Section titled “Transient stress changes the termination ranking”All four architectures targeted 800 V under DC conditions. The unterminated, field-plate-only, and JTE-only devices could not sustain the short voltage spike. Breakdown was extracted at the onset of avalanche, identified by a sharp reverse-current increase and an impact-ionization integral above unity. Dynamic results also showed that previously optimized JTE designs degraded more than configurations with detuned parameters. Under slow ramps, the JTE controlled blocking. Under fast ramps, field-plate parameters controlled it.
Modeling sequence and device assumptions
Section titled “Modeling sequence and device assumptions”The workflow used mixed-mode TCAD, solving the external circuit and internal device physics together at each time step. It began with a 1 V/s quasi-static reverse ramp for a baseline blocking voltage and geometry ranking. It then applied isothermal ramps or square waveforms from 1 V/s to 10^6 V/s to expose charge-redistribution effects. The final step solved Poisson, carrier transport, and heat-flow equations self-consistently to include self-heating.
The baseline used a one-dimensional parallel-plane breakdown limit calculated with Hiraiwa’s impact-ionization coefficients. For a target breakdown voltage of approximately 1200 V, the selected drift layer used an acceptor concentration of 5 × 10^16 cm^-3. Its epitaxial thickness was 2 µm, near the transition between punch-through and non-punch-through operation. This placement allowed full drift depletion at breakdown while limiting drift resistance.
Most devices reported in the literature reached less than 60% of the theoretical limit. The authors state that reverse-bias failure remained dominated by material and processing limits rather than avalanche-limited breakdown.
| Device parameter | Simulated value |
|---|---|
| p-type drift layer | N_A = 5 × 10^16 cm^-3 |
| Epitaxial layer | 2 µm |
| Phosphorus JTE | N_D = 1 × 10^18 cm^-3; thickness 200 nm |
| Thermal substrate | 300 µm type-Ib diamond |
| Backside boundary | 0.3 K/W thermal resistance; other boundaries adiabatic |
The three termination geometries were optimized with routines reported in earlier diamond studies.
Delayed donor ionization causes premature avalanche
Section titled “Delayed donor ionization causes premature avalanche”Phosphorus has a donor ionization energy of 0.57 eV. At room temperature, less than 1% of donors were ionized when N_D exceeded 10^15 cm^-3. The ionization time constant ranged from 1 ms to 10 s, depending on the phosphorus capture cross-section.
At 10 to 10^2 V/s, complete and incomplete ionization produced comparable reverse-current responses. Both cases showed displacement current during the rise, then returned to dark current at 1100 V. At 10^4 to 10^6 V/s, incomplete ionization produced a sharp current rise consistent with avalanche. The current then relaxed toward dark current over a period equal to the donor ionization time constant.
Under full ionization, displacement current only increased in proportion to the shorter rise time. Under incomplete ionization, too few ionized donors could support the reverse bias. As voltage rose, donors ionized around the junction, and electrons from neutral donors entered the high-field region. This process increased impact ionization and lowered the effective avalanche threshold.
After more than 1 ms at full ionization, the peak field remained at the pn-junction interface. With incomplete ionization, field crowding appeared at the Schottky-contact edge and could exceed diamond’s critical field under optimistic assumptions. A JTE that appears effective under DC conditions can therefore fail early during a fast reverse transient.
Hybrid termination controls field redistribution
Section titled “Hybrid termination controls field redistribution”The hybrid design combined a 200 nm phosphorus-doped JTE with an Al2O3 field plate. The authors selected Al2O3 because it offered one of the best trade-offs and was the most experimentally validated oxide for diamond devices. SiO2, ZrO2, and other high-k dielectrics were described as promising candidates.
The field plate carried the early transient, while the JTE took over as donor ionization recovered. The hybrid then behaved progressively like a JTE as the field settled toward its quasi-static value. Field-plate action dominated during the initial pulse, while the JTE became effective after recovery exceeded the ionization time constant. This complementary action maintained high blocking efficiency over a broad voltage slew-rate range.
Self-heating changes recovery and loss
Section titled “Self-heating changes recovery and loss”Electrothermal simulations used a 10^6 V/s pulse that saturated at 1.1 kV. Initial lattice temperatures were 278 K, 298 K, and 398 K.
The hybrid showed no significant self-heating because its terminated region handled low power density from low leakage current. The JTE-only device rose approximately 20 K from room temperature. Heating was localized near the Schottky-contact edge because of field crowding and avalanche-induced self-heating. At 398 K, self-heating was fully mitigated because diamond’s critical field increased with temperature under the impact-ionization model.
Higher junction temperature increased the donor ionization ratio, speeding current recovery toward the steady dark current. Moderate heating temporarily shortened the current increase during turn-off. It also increased turn-off losses, which could limit maximum power and switching frequency. The avalanche current lasted briefly, so different thermal impedance networks had little effect on the electro-thermal response.
Oxide stress and model limits
Section titled “Oxide stress and model limits”The hybrid reduced surface stress, but it transferred some peak field into the dielectric. During the early pulse, oxide field increased until the JTE recovered. The field then settled below the field-plate-only value.
The authors expect lower oxide fields to reduce leakage and lengthen oxide and device lifetimes. That lifetime benefit remains a model-based expectation because the analysis excluded premature oxide breakdown. The simulation modeled only avalanche breakdown. Omitting oxide failure can overstate field-plate efficiency, although the termination ranking should hold if oxide thickness withstands the elevated surface fields.
The normalized peak field of approximately 25 MV/cm was a numerical reference, not a strict physical limit. The field ratios compare JTE-only with hybrid in diamond and FP-only with hybrid in oxide.
The study explored rates to 10^6 V/s, while automotive SiC and GaN converters can reach 10^9 to 10^10 V/s. The authors state that diamond’s transient limitations were fully developed at rates beyond 10^6 V/s, so higher rates did not qualitatively change breakdown.
Fabrication of the 200 nm n-type layer at 10^18 cm^-3 also remains challenging. All hybrid results were simulated, without a prototype test or an oxide-lifetime measurement.
Implications for diamond device selection
Section titled “Implications for diamond device selection”Transient modeling should therefore be part of edge-termination selection, rather than relying on quasi-static breakdown voltage alone. For the automotive architecture, the hybrid had the highest modeled likelihood of withstanding the transient overvoltage. The field plate handles the early voltage transition, and the JTE regains control after donor ionization recovers.
Oxide thickness and geometry must provide enough dielectric margin for the temporary field transfer. The hybrid approach also offered fixed-footprint robustness relative to a field-plate-only design. Device engineers should also check that the required thin, highly doped n-diamond layer can be fabricated reproducibly. Otherwise, the simulation supports a promising termination concept, not an experimental qualification of a 1200 V diode.
Materials and support
Section titled “Materials and support”The modeled Schottky barrier diode requires a 300 µm type-Ib diamond substrate, a phosphorus-doped JTE, and an Al2O3 field plate. 6CCVD’s diamond materials catalog lists MPCVD-grown single-crystal diamond from 0.1 to 500 µm thick, which includes the modeled 300 µm substrate thickness. The linked engineering support service can be used to define custom fabrication work for the device-specific epitaxy and termination.
View Original Abstract
Traditional design and optimization of Si-based power devices rely on quasi-static edge termination modeling that has proven to be effective in reproducing experimental results. However, this approach fails to accurately describe emerging wide- and ultra-wide bandgap (UWBG) power devices operating in fast-switching environments, such as in automotive applications, where devices are subject to rapid voltage and over-current transients ($\textit {dV}/\textit {dt} \gt 100$V/ns). The absence of a robust design methodology that captures the transient electro-thermal response of the semiconductor, oxide, and passivation layers often results in devices that underperform in real operating conditions. This work addresses this longstanding challenge by introducing a comprehensive dynamic simulation framework that reproduces key aspects of dynamic reverse-bias (DRB) testing used for automotive qualification. Using a diamond-based Schottky barrier diode (SBD) as a case study, we demonstrate that conventional quasi-static and time-dependent simulation strategies lead to markedly different design outcomes. The proposed transient approach captures the interplay between field redistribution, charge trapping, and self-heating effects, offering enhanced predictive accuracy and robustness for the next generation of power devices.
Boron Doped Single Crystal Diamond Plate
View Specs →
Advanced Thermal Simulation Service Diamond Heat Spreader Performance Analysis
View Specs →
Single Crystal Cvd Diamond Plate
View Specs →Original source
Section titled “Original source”References
Section titled “References”- 2018 - 6.2 diamond devices in power converters: Needs