Skip to content

Electrochemical Sensor of Ciprofloxacin on Screen-Printed Electrode Modified with Boron-Doped Diamond Nanoparticles and Nickel Oxide Nanoparticles Biosynthesized Using Spatholobus littoralis Hassk. Root Extract

FieldValue
JournalBiosensors
Published2026-03-03
AuthorsLaurencia Gabrielle Sutanto, Prastika Krisma Jiwanti, Mirza Ardella Saputra, Mai Tomisaki, Nurul Mutmainah Diah Oktaviani
DOI10.3390/bios16030148

Adding nickel oxide nanoparticles to a boron-doped diamond nanoparticle-modified screen-printed electrode lowered the ciprofloxacin detection limit to 0.054 µM. The combined sensor gave a linear buffer response over 0.1 to 100 µM. The combined sensor returned 98.11% to 99.59% recovery in 100 µM tablet, milk, and urine tests.

The authors compared an unmodified screen-printed electrode with BDD NPs/SPE and NiO NPs/BDD NPs/SPE. BDD NPs/SPE contained boron-doped diamond nanoparticles only. NiO NPs/BDD NPs/SPE added nickel oxide nanoparticles over that layer. Both electrodes used a three-electrode configuration with a 0.5 cm working electrode. The BDD ink contained 10 mg of powder in 0.5 mL of 30% ethanol. The commercial powder was specified as 0 to 250 nm. A 4 µL drop of BDD ink was placed on the working electrode and dried at 50 °C for 5 min. A 4 µL drop of NiO nanoparticle solution was then placed on the BDD-coated electrode and dried under the same conditions. SEM showed polycrystalline BDD nanoparticles covering the porous electrode. NiO particles were distributed over the BDD-coated surface, and SEM-EDX confirmed successful modification.

They boiled 10 g of dried root powder in 100 mL of 40% methanol at 80 °C for 30 min. The filtered extract was stored at 4 °C for later synthesis. The extract was mixed with 100 mL of 0.1 M NiCl2 at a stated 50% v/v ratio. A 5 M NaOH solution raised the pH to 12, followed by heating and stirring at 60 °C for 60 min. Centrifugation at 4000 rpm for 15 min separated the precipitate. The precipitate was washed three times with absolute ethanol and dried at 80 °C for 12 h. For XRD, the powder was calcined at 400 °C for 2 h. DLS measured particles from 56 to 95 nm, with an average of 73 nm and a polydispersity index of 0.261. UV-Vis showed a maximum near 296 nm. After 25 days at 4 °C, absorbance fell 8.21% and the peak shifted to 302 nm. The authors treated the 25-day change as evidence that the stored particles remained stable. Five sharp XRD peaks were assigned to the NiO (111), (200), (220), (311), and (222) planes. XRD also indicated a face-centered cubic phase and a calculated crystallite size of 0.69 nm. XPS identified both Ni2+ and Ni3+ states, while SEM showed spherical particles. The authors associated FT-IR changes with reduction of Ni2+ and oxidation of extract compounds. EDX detected carbon, oxygen, and nickel in the product.

Electrochemical response and scan-rate behavior

Section titled “Electrochemical response and scan-rate behavior”

Electrochemical measurements used 0.1 M phosphate buffer at pH 7.0. Square-wave voltammetry used a range of 0 to 1.2 V versus Ag/AgCl at 50 Hz. The amplitude was 0.05 V, and the potential step was 0.012 V. CV of 100 µM ciprofloxacin, abbreviated CIP, showed an anodic peak near 0.85 V. The NiO-containing electrode produced a larger CIP peak current than the BDD-only electrode. The authors linked this result to better electrical conductivity with NiO. The SWV signal-to-background ratio rose from 23 for BDD NPs/SPE to 36 for the combined electrode. They attributed the increase to a larger CIP peak current and a lower background current. CV used scan rates from 20 to 100 mV/s with 100 µM CIP. Log current increased linearly with log scan rate for both electrodes. The slopes were 1.103 for BDD NPs/SPE and 1.225 for the combined electrode. Both values led the authors to classify CIP detection as adsorption controlled. The proposed oxidation route forms an N-hydroxylation derivative from CIP’s secondary amine group through loss of two protons and two electrons. The authors presented that reaction as plausible rather than directly proven.

Calibration, detection limits, and selectivity

Section titled “Calibration, detection limits, and selectivity”

Peak current increased with CIP concentration across 0.1 to 100 µM. For BDD NPs/SPE, Ip in µA equaled 3.973 C + 105.789, with R² = 0.998. For NiO NPs/BDD NPs/SPE, Ip in µA equaled 4.404 C + 419.282, with R² = 0.999. Both equations use C in µM and Ip in µA. The combined electrode had the higher calibration slope. LOD and LOQ used the blank standard deviation from three measurements and the calibration slope.

The calibration and background results below used 0.1 M phosphate buffer at pH 7.0.

ElectrodeLinear range (µM)LOD (µM)LOQ (µM)S/B
BDD NPs/SPE0.1 to 1000.1090.36523
NiO NPs/BDD NPs/SPE0.1 to 1000.0540.18236

Selectivity tests added 100 µM D-glucose, 60 µM levofloxacin, 60 µM ofloxacin, 60 µM ascorbic acid, 4 µM NaCl, and 10 µM urea. Both electrodes kept the CIP peak distinguishable from those interferents. Urea, ascorbic acid, and NaCl produced peaks near +0.5 V, although the authors suggested electrode impurities as a possible source.

Precision, reproducibility, and real samples

Section titled “Precision, reproducibility, and real samples”

Reproducibility was tested over nine consecutive days with different electrodes. The BDD-only electrode averaged 489.945 ± 1.676 µA, with an RSD of 0.348%. The combined electrode averaged 810.465 ± 2.003 µA, with an RSD of 0.247%. Repeatability used seven measurements on one electrode during one day. The corresponding RSD values were 0.111% and 0.107%. These values were below the paper’s 2% reliability criterion. Commercial tablets were dissolved and diluted to 100 µM. Cow’s milk and human urine were spiked with 100 µM CIP in 0.1 M phosphate buffer at pH 7.0.

Recovery results for the 100 µM real-sample tests are shown below.

SampleCIP level (µM)BDD NPs/SPE recoveryNiO NPs/BDD NPs/SPE recovery
Tablet10096.50%99.39%
Milk10095.13%98.11%
Human urine10098.61%99.59%

Comparison with prior ciprofloxacin sensors

Section titled “Comparison with prior ciprofloxacin sensors”

The combined electrode had the lowest detection limit in the paper’s comparison table. It covered 0.1 to 100 µM, wider than most listed methods. GO/SPE used DPSV and reported an LOD of 0.30 µM over 1 to 8 µM. The rGO-SnO2/SPE used SWV and reported an LOD of 2.03 µM over 30 to 100 µM. The molecularly imprinted Ch-AuMIP/GCE electrode reported 0.21 µM over 1 to 100 µM. The paper-based electrode reported 4.96 µM over 9.9 to 220 µM. CRGO/GCE and MIP/GCE had detection limits of 0.21 and 11.2 µM, respectively. The BDD-only electrode also reached 0.109 µM, below every prior detection limit listed in the table. Detection limits alone do not establish equivalent matrix performance, reproducibility, or selectivity across these studies.

The study did not evaluate pH systematically. All electrochemical work used near-neutral phosphate buffer at pH 7.0. Performance in acidic or alkaline matrices therefore remains untested. Real-sample validation used one 100 µM level for each matrix. The urine came from one healthy volunteer, so patient-to-patient variability was not tested. The paper reports fixed-concentration interferent tests, not separate matrix-interference studies. The 25-day stability result applies to stored NiO powder, not a complete modified electrode. The authors proposed therapeutic drug monitoring, but their reported matrices were tablets, milk, and urine. For electrode development, the measured data favor combining NiO with BDD nanoparticles rather than using the BDD-only modifier. This choice applies to the near-neutral pH and single-level real-sample conditions tested here. Additional validation is needed for other matrices, pH values, and routine clinical testing.

This sensor needs boron-doped diamond nanoparticles in a drop-castable ink for a screen-printed working electrode. The paper used 0 to 250 nm commercial powder, and the 6CCVD diamond materials catalog lists boron-doped diamond. The engineering support page can be used to check particle-form suitability for this ink.

View Original Abstract

Ciprofloxacin (CIP) is an antibiotic that is widely used in humans and animals. However, the compound has been detected in animal-derived products and the environment due to its extensive use, causing serious concern for public health and environmental safety. The issue raises the urgent need to develop innovative techniques to monitor CIP. Therefore, this study aims to develop a simple and sensitive CIP sensor called the boron-doped diamond nanoparticle-modified screen-printed electrode (BDD NPs/SPE) and the nickel oxide nanoparticle-modified BDD NPs/SPE (NiO NPs/BDD NPs/SPE). NiO NPs were synthesized via green synthesis using Spatholobus littoralis Hassk. root extract as the reducing agent. The formation and characteristics of NiO NPs were then confirmed through a UV-Vis spectrophotometer, XRD, PSA, FT-IR, and XPS. The successful modification of SPE was confirmed through SEM-EDX, followed by measurements using square-wave voltammetry. The results showed that the modified SPE could detect CIP over a concentration range of 0.1-100 µM and produced a low detection limit of 0.109 µM for BDD NPs/SPE and 0.054 µM for NiO NPs/BDD NPs/SPE. The proposed method was successfully applied to the determination of CIP in commercial tablets, milk, and human urine, with a satisfactory % recovery from 95 to 100%. The current study successfully developed a simple yet highly sensitive sensor that enabled robust, reliable, and efficient detection of CIP, showing its strong potential for practical applications.

  1. 2018 - Ciprofloxacin Derivatives and Their Antibacterial Activities [Crossref]
  2. 2018 - Highly Sensitive Immunochromatographic Detection of Antibiotic Ciprofloxacin in Milk [Crossref]
  3. 2021 - Adsorption of Ciprofloxacin from Water: A Comprehensive Review [Crossref]