Hierarchical Structured TiO 2 /Boron‐Doped Diamond for Efficient Photo‐Electrocatalytic Degradation
Paper details
Section titled “Paper details”| Field | Value |
|---|---|
| Journal | Rare Metals |
| Published | 2026-05-01 |
| Authors | Haiming Sun, Peng Li, Xi Zhang, Yuxiao Liu, Jinfei Zhao |
| DOI | 10.1002/rar2.70301 |
Only 9.4% of Reactive Blue 21 remained after 300 min of photoelectrochemical treatment with a TiO2 array on boron-doped diamond. The reported optimum used 0.1 M Na2SO4, pH 3, and 15 mA cm−2. The degradation rate was 2.32 times that of fully coated TiO2/BDD and 1.57 times that of bare BDD. Exposed BDD supplied oxidation sites between the TiO2 features.
Patterned TiO2 leaves BDD available for oxidation
Section titled “Patterned TiO2 leaves BDD available for oxidation”The titanium dioxide array, or TiO2-AR, covered about 60% of a 10 mm × 10 mm × 1 mm boron-doped diamond substrate. Each TiO2 feature was about 2 mm in diameter. Cross-section SEM measured a film thickness of 147.4 nm. This pattern left BDD exposed between the photocatalytic regions. The authors designed it to limit the electrochemical blocking caused by a continuous TiO2 coating.
Fabrication began with cleaning and drying the BDD. A mask plate and the substrate were mounted for magnetron sputtering. The chamber was held at 2 × 10−3 Pa, and the substrate was heated to 300°C. Argon and oxygen entered at 15 sccm each. A 300 W RF source sputtered a high-purity titanium target for 120 min. The coated electrode was annealed at 450°C for 180 min to crystallize TiO2. The control electrode carried a continuous TiO2 layer over the BDD.
Surface characterization confirms anatase TiO2 on diamond
Section titled “Surface characterization confirms anatase TiO2 on diamond”X-ray diffraction identified the anatase TiO2 (101) reflection at 25.3°. Diamond reflections appeared at 43.9° and 75.3°, corresponding to the (111) and (220) planes. EDS mapping showed uniform Ti and O distributions in the top layer and a carbon-rich BDD layer below. The XPS O 1s peak at 530.0 eV was assigned to lattice oxygen. Ti 2p peaks at 458.8 and 464.5 eV differed by 5.7 eV and indicated Ti4+. The coated surface also lowered the contact angle from 87.2° to 36.0°.
The array shifts the photoelectrochemical response
Section titled “The array shifts the photoelectrochemical response”The PEC tests used a three-electrode cell with an Ag/AgCl reference and a platinum counter electrode. A 150 W xenon lamp illuminated the working electrode without wavelength selection. Photocurrent and linear sweep voltammetry were measured in 0.1 M Na2SO4 at 50 mV s−1. CV used a 0.01 M K3Fe(CN)6/K4Fe(CN)6 mixture with 0.1 M Na2SO4 at the same scan rate.
| Measurement | TiO2-AR/BDD | TiO2/BDD | Bare BDD |
|---|---|---|---|
| Photocurrent at 1.5 V, mA cm−2 | 0.46 | 0.25 | Not reported |
| Dark current at 1.5 V, mA cm−2 | 0.34 | Not reported | Not reported |
| Illuminated oxidation peak current, mA cm−2 | 0.34 | 0.11 | Not reported |
| Charge transfer resistance in dark, Ω | 2,000 | 6,100 | 300 |
| Charge transfer resistance under light, Ω | 800 | 4,000 | Not reported |
At 0.5 V and 1.0 V, fully coated TiO2/BDD produced higher photocurrent than the array. The authors attributed this to its larger photocatalytic area because the bias had not reached BDD oxidation. At 1.5 V, the dense TiO2 film carried almost no dark current. The array maintained an active anodic response through its exposed BDD regions.
Under illumination, the array retained a defined oxidation response from the exposed BDD. Illumination lowered charge transfer resistance for both composites, with the array remaining below the full coating. The TiO2 layer showed a rectification ratio of roughly 171, which the authors used as evidence for a BDD-TiO2 junction. They attributed charge separation to the internal field between TiO2 and H-terminated diamond. The reported band gaps were about 3.3 eV for TiO2 and 5.5 eV for H-terminated diamond. Photocurrent transients at 1.5 V were slow because hole arrival at the surface exceeded hole consumption.
Operating conditions control RB21 removal
Section titled “Operating conditions control RB21 removal”Section 3.3 states that the degradation tests used 2 cm × 2 cm electrodes, a 1.5 cm interelectrode distance, and 400 rpm stirring. Samples came from 250 mL of simulated wastewater. RB21 concentration was measured by UV-visible absorbance at 625 nm using a calibration spanning 0 to 50 mg L−1. Each condition was repeated three times and averaged.
At 0.1 mol L−1 electrolyte, 10 mA cm−2, pH 7, and 240 mg L−1 initial RB21, NaCl left 4.55% RB21 after 300 min. Na2SO4 left 7.87%, while NaNO3 left 55.46%. The authors chose Na2SO4 for later tests. Chloride oxidation formed reactive chlorines but could also generate chlorite, chlorate, and perchlorate.
Each one-factor series changed one setting while holding its remaining settings fixed. Separate Na2SO4 concentration tests gave residual RB21 fractions of 18.99%, 9.20%, and 3.98%. The corresponding sulfate concentrations were 0.02, 0.05, and 0.1 mol L−1. The pseudo-first-order rate constants were 5.74 × 10−3, 8.01 × 10−3, and 11.96 × 10−3 min−1, respectively.
At pH 3, 7, and 11, residual RB21 was 4.46%, 12.65%, and 23.46%. The corresponding rate constants were 11.03 × 10−3, 7.16 × 10−3, and 5.31 × 10−3 min−1. The TiO2 point of zero charge is about 6.2. Below that value, positive TiO2 attracts anionic RB21 through its sulfonate group. Above it, electrostatic repulsion limits mass transfer.
At 5, 10, and 15 mA cm−2, residual RB21 was 16.57%, 7.88%, and 3.76% after 300 min. The radar analysis identified current density as the strongest of the four tested variables. The authors warned that excess current favors oxygen evolution. Bubble formation can reduce Faradic efficiency and electrode stability.
Under the optimum used above, bare BDD left 42.43% RB21. The fully coated TiO2/BDD electrode left 60.9%. The array combined exposed BDD oxidation with TiO2 photocatalysis. The dense coating restricted BDD access, while bare BDD lacked a photocatalytic component.
Hydroxyl radicals drive the measured pathway
Section titled “Hydroxyl radicals drive the measured pathway”Methanol quenches hydroxyl radicals, sulfate radicals, and other oxidative species. Tert-butanol mainly quenches hydroxyl radicals because its reaction with hydroxyl radicals is about 1,000 times faster than its reaction with sulfate radicals. Adding 0.1 M methanol left 71.27% RB21. Adding 0.1 M tert-butanol left 64.38%. The authors assigned the main oxidation role to hydroxyl radicals and an auxiliary role to sulfate radicals.
ESR detected DMPO-hydroxyl radical adducts for all three electrodes. The characteristic peaks were strongest for TiO2-AR/BDD. Positive-mode HPLC-MS supported a pathway that begins with peripheral C-N bond and sulfonate group cleavage. The sequence then includes deamination, aromatic rearrangement, ring opening, smaller fragments, and an inorganic P14 product. Carbon dioxide and water are the stated final products.
DFT calculations used the B3LYP functional and 6-31G(d, p) basis set. Fukui indices ranked several peripheral carbon and nitrogen sites as likely radical attack positions. ECOSAR estimated acute LC50 and chronic ChV values for fish, Daphnia, and green algae. The model classified initial RB21 as highly acutely toxic to all three organisms. Ring-opening products P4, P5, P7, and P11 were classified as non-toxic for acute toxicity, although some small products retained chronic toxicity. These toxicity results are model estimates rather than biological measurements.
Total organic carbon removal was 86.85%, while chemical oxygen demand removal was 90.25%. TOC samples were quenched with 10% Na2SO3 before analysis. COD used the standard dichromate closed-reflux method. The authors expected the remaining small intermediates to undergo further mineralization.
Limits for device and process development
Section titled “Limits for device and process development”The study treated one dye in 250 mL of simulated wastewater. It does not establish removal of mixed contaminants or real textile effluent. The 150 W xenon source had no wavelength selection, so the illumination spectrum was not tightly specified.
Postreaction SEM and XRD showed no significant changes in morphology or crystal phase. The paper does not report accelerated lifetime testing, electrode cycling, or large-area coating uniformity. These results establish short-term structural stability under the reported test, not long-term service life.
The cell description is also inconsistent. Section 2.1 specifies a 20 mm × 20 mm × 1 mm stainless steel cathode. Section 3.3 describes 2 cm × 2 cm electrodes as both anode and cathode. That discrepancy must be resolved before reproducing the reactor.
The study tested one TiO2 coverage and feature size. Device selection must balance exposed BDD oxidation area against TiO2 photocatalytic area. Production geometry should also qualify gas evolution and electrode lifetime. A dense TiO2 coating should not be assumed to maximize PEC treatment when BDD oxidation remains active.
Materials and support
Section titled “Materials and support”The paper requires a boron-doped diamond anode substrate for masked TiO2 deposition and exposed electrochemical oxidation sites during RB21 treatment. 6CCVD’s diamond materials catalog offers MPCVD-grown single-crystal and polycrystalline diamond and boron-doped diamond. Custom fabrication support for defining the TiO2 pattern and electrode integration can be discussed through engineering support.
View Original Abstract
ABSTRACT The discharge of refractory organic dye wastewater poses a significant threat to the ecological environment, necessitating the development of efficient treatment technologies. Herein, a uniform TiO 2 array (TiO 2 ‐AR) electrode is fabricated using a combination of magnetron sputtering and a mask plate process with a boron‐doped diamond (BDD) substrate for Reactive Blue 21 organic wastewater treatment. Photo‐electrochemical (PEC) measurements were conducted to evaluate the photo‐electrochemical behaviors of TiO 2 ‐AR, the TiO 2 ‐BDD electrode with a full layer of TiO 2 on the BDD substrate, and the pure BDD electrode. The PEC results show that the TiO 2 ‐AR/BDD electrode significantly outperforms both the TiO 2 /BDD electrode and the BDD electrode. The degradation rate of RB21 simulated wastewater by the TiO 2 ‐AR/BDD electrode is 2.32‐fold and 1.57‐fold higher than that by the TiO 2 /BDD electrode and the BDD electrode, respectively. The radical quenching experiments verify that hydroxyl radicals (•OH) are the main reactive oxygen species responsible for the degradation of RB21. The reaction pathways for the degradation of RB21 are then confirmed by HPLC‐MS and theoretical calculations. Moreover, the toxicity of the degradation intermediate of RB21 is estimated quantitatively with a quantitative structure‐activity relationship (QSAR), faithfully evidencing that both acute and chronic toxicities were effectively decreased after degradation. This work presents an efficient surface modification approach that integrates photocatalysis and electrocatalysis synergistically for wastewater treatment.
Boron Doped Diamond On Titanium Bdd Electrode
View Specs →
Boron Doped Single Crystal Diamond Plate
View Specs →