Skip to content

Widefield NV magnetic field reconstruction for probing the Meissner effect and critical current density under pressure

FieldValue
JournalApplied Physics Letters
Published2026-05-25
AuthorsKin On Ho, Cassandra Dailledouze, Martin Schmidt, Loïc Toraille, Marie‐Pierre Adam
DOI10.1063/5.0323142

Widefield NV magnetometry reconstructed the magnetic field around an HgBa2Ca2Cu3O8+δ microcrystal at approximately 4 GPa. The authors report the first widefield quantitative reconstruction of field screening under pressure. The reconstructed profile gives a critical current density of about 1.5 × 10^4 A·cm⁻² at 120 K and approximately 4 GPa. That value agrees with the cited ambient-pressure range of roughly 1 × 10^4 to 10^5 A·cm⁻² at slightly lower temperatures.

The Hg-1223 microcrystal had a critical temperature of about 138 K under pressure. The reconstruction separated superconducting behavior below this transition from normal-state behavior above it.

At 120.8 K and 135.2 K, the reconstructed field magnitude and polar angle varied strongly across the sample. At 149.9 K, both became nearly uniform. The maps therefore resolved the local field signature of screening rather than measuring only a bulk magnetic response.

The experiment placed the Hg-1223 microcrystal beside an NV-doped [100]-cut diamond in a diamond anvil cell. The sample c axis and applied field B0 were aligned with the diamond [001] direction. A zero-field-cooling followed by field-warming procedure was used.

Excitation used a laser power of 34.7 mW, microwave power of 20 dBm, and an applied field of 3 mT. Widefield maps were recorded at increasing temperatures. The dataset contained about three million data points. The authors reduced it to about twenty-five thousand points using one vertical line cut, one horizontal line cut, and a square around the sample.

The ODMR spectrum encodes the field vector through its projections onto the four NV axes. The authors fitted these spectra with solutions of the NV ground-state Hamiltonian and the relative contrast of the resonances. The longitudinal zero-field splitting D depends on temperature and pressure. The Zeeman coefficient was 28 MHz/mT, and hyperfine structure was irrelevant within the measurement range.

The initial model had eight parameters. They described field magnitude, polar angle, azimuthal angle, contrast modulation εB, Lorentzian contrast C, linewidth δν, pressure P, and stress parameter α. The authors fixed α at 0.45 for an initial pressure near 4 GPa. They fitted δν above the critical temperature, leaving six free parameters for the main fit.

The model treats the microwave field as an amplitude modulation of the static field because the microwave wavelength exceeded the sample dimensions. It assumes the expelled microwave field remains aligned with the local expelled static field. The α parameter represents stress deviations from hydrostatic pressure caused by cupping of the anvil tip.

Fits were constrained to evolve smoothly across position and temperature. Each fitted result supplied starting conditions for the next fit. This procedure imposed a self-consistent field evolution over the mapped area.

The reconstructed vectors show strong bending above and beside the microcrystal. At low temperature, the field magnitude falls and its direction turns sharply. Near the center in the superconducting state, the magnitude reaches about 0 mT.

As temperature rises toward the critical temperature, vectors near the center point back toward the sample c axis and regain magnitude. Edge vectors lose magnitude with only a small angular change. These features support the diamagnetic Meissner response.

The field changes rapidly between 135.2 K and 137.6 K. Region I shows the sharpest profile change at the top of the vertical cut, correlated with the sharpest sample edge. Region II contains the lowest field, which the authors attribute to the shortest distance between the NV centers and the sample.

Region III retains a finite field inside the sample. The authors relate this residual field to flux penetration through a defect identified in their previous analysis. The irregular sample shape also produced different profiles at the two ends of the vertical cut.

The authors fitted the reconstructed transverse field profile with Brandt’s model for a type-II superconductor. The model geometry was a semi-infinite slab with width 2w and thickness t, where w was much larger than t. The external field was applied perpendicular to the slab.

Critical current density jc was the only fitted parameter. The parameter β describes the lateral penetration depth of the magnetic field. The parameter γ gives the ratio between B0 and the surface field induced by the critical sheet current Jc = jct.

Line-cut fits were shown at 124.4 K, 129.5 K, and 136.8 K. The sharp positive x edge set the best fit, which was then compared with the negative x side. The experimental data were slightly scattered but largely followed Brandt’s model.

Critical current density increased as the sample cooled. Near the critical temperature, β had exponential sensitivity in the low-jc regime. A modest temperature change therefore redistributed the magnetic field around the superconductor. At temperatures well below the critical temperature, β approached saturation and screening became weakly temperature dependent.

Earlier Brandt analyses used NV splitting without a detailed field map. The paper notes that splitting alone could not describe the phase transition completely. The new fit uses the reconstructed profile, although the microcrystal does not match the ideal slab geometry exactly.

Estimated uncertainty is below ±0.1 mT for field magnitude. Polar-angle uncertainty is about ±5°, and azimuthal-angle uncertainty is about ±10°. The Gaussian excitation profile and nonuniform microwave field cause spatial dependence in the data.

Pressure also varies across the cell. Direct contact between Hg-1223 and the diamond produces a higher local pressure. This variation means that a single nominal pressure does not describe every sensing position.

The Brandt fit ignores the minimum 20 nm standoff caused by NV implantation depth. Finite spatial resolution and the absence of sharp sample edges smooth the field changes used in the fit. The irregular sample also differs from the ideal slab model.

The authors suggest machine learning or artificial intelligence could refine the model and reconstruct the field vector over the full map. Those methods remain proposed improvements rather than demonstrated results in this study.

The reconstruction extracts jc under pressure without relying on electrodes for high-pressure transport measurement. It separates field magnitude from orientation instead of using ODMR splitting alone.

The paper identifies the [100] diamond orientation and implanted-layer depth as experiment-specific sensor requirements. Its analysis also shows that spatial resolution and sample-edge geometry affect the extraction of jc.

Combined with previous measurements of the lower and upper critical fields, Hc1 and Hc2, the authors conclude that NV magnetometry can determine three critical superconducting parameters under pressure.

The sensing element for this high-pressure magnetometry application is NV-doped, [100]-cut single-crystal diamond with an implanted layer positioned close to the Hg-1223 microcrystal. The diamond materials catalog includes MPCVD-grown single-crystal diamond plates and wafers up to 125 mm, providing the base material family for this sensor. The paper’s [100] cut and NV implantation requirements should be confirmed with 6CCVD’s engineering support.

View Original Abstract

The spatial distribution of a magnetic field can be determined with micrometer resolution using widefield nitrogen vacancy (NV) center magnetic imaging. Nevertheless, reconstructing the magnetic field from the raw data can be challenging due to the degeneracy of the four possible NV axes and the tremendous amount of data. While a qualitative approach is sufficient for most analyses, a quantitative analysis offers deeper insight into the physical system. Here, we apply NV widefield magnetic imaging to a HgBa2Ca2Cu3O8+δ (Hg-1223) superconducting microcrystal at a pressure of 4 GPa. We fit the results with solutions from the Hamiltonian describing the NV center ground state and take into account the relative intensities of the resonances to determine the local magnetic field magnitude and angle. Thus, we reconstruct the temperature-dependent expulsion of the magnetic field associated with the Meissner effect around the superconductor. By comparing the resulting parameters to Brandt’s model, which describes the magnetic behavior of a type-II superconductor, we extract the critical current density jc. Overall, this work showcases the first widefield quantitative reconstruction of the field screening under pressure and an optical method to study critical current density. Thus, it provides new insights into the application of NV magnetometry to superconductivity research at high pressures.