High-Gain Hydrogen-Terminated Diamond Logic Circuits With Low Power-Consumption
Paper details
Section titled “Paper details”| Field | Value |
|---|---|
| Journal | IEEE Electron Device Letters |
| Published | 2026-06-12 |
| Authors | Lei Ge, Siying Gao, Xuemin Zhao, Mingyang Wang, Yaxin Li |
| DOI | 10.1109/led.2026.3701759 |
Normally off Al/BaF2/H-diamond FETs produced an inverter with a peak voltage gain of -460 V/V at VDD = -5 V and static power of about 1 pW. The paper reports this as the highest gain for a diamond inverter. It also reports the first experimental diamond ring oscillator. Both results were measured at room temperature.
Logic design and headline result
Section titled “Logic design and headline result”Each inverter used two p-channel MISFETs, with the 5 µm device as the driver and the 1 µm device as the load. The load gate was shorted to its source, and both gate widths were 50 µm. The measured threshold voltages were -1.1 V for the driver and -0.3 V for the load.
A low input kept the driver on and pulled Vout to GND. Between -1.1 V and 0 V, the driver turned off and Vout fell to VDD. This arrangement separated the switching states of the two devices. The authors attributed the low static power to the well-matched, normally off transistor characteristics.
Diamond layer and gate stack
Section titled “Diamond layer and gate stack”The starting material was a 10 × 10 × 1 mm³ high-pressure, high-temperature single-crystal diamond substrate. After chemical mechanical polishing, an acid mixture removed the non-diamond phase and metal ions. A 150 µm undoped single-crystal thin film was then grown by microwave plasma chemical vapor deposition.
Hydrogen termination followed in a hydrogen plasma for more than 15 minutes at 900 °C without methane. The sample was cooled in the hydrogen atmosphere. An 80 nm Au film was deposited to protect the two-dimensional hole gas and form an ohmic contact.
Source and drain pads were patterned by photolithography, and the Au was wet-etched with an aqueous KI/I2 solution. Surface isolation used 15 minutes of UV exposure in ozone to convert C-H bonds into C-O bonds. The 30 nm BaF2 dielectric and 100 nm Al gate were thermally evaporated at room temperature under 5 × 10⁻⁶ torr background vacuum. Al interconnections were deposited by evaporation and lift-off. Electrical characterization used a probe system at room temperature.
Transistor characteristics
Section titled “Transistor characteristics”Output measurements swept VG from 0 to -4 V in 0.5 V steps while VD ran from 0 to -5 V. Transfer measurements swept VG from 1 V to -4 V at VD = -5 V.
| Parameter | 1 µm FET | 5 µm FET | Measurement condition |
|---|---|---|---|
| Maximum drain current density | -166 mA/mm | -67 mA/mm | VG = -4 V, VD = -5 V |
| Normalized on-resistance | 16.7 Ω·mm | 34.7 Ω·mm | VG = -4 V |
| Threshold voltage | -0.3 V | -1.1 V | Linear-region extrapolation at VD = -5 V |
| Maximum extrinsic transconductance | 70.6 mS/mm | 34.1 mS/mm | Transfer characteristics at VD = -5 V |
| On/off ratio | Above 10^10 | Above 10^10 | Transfer sweep at VD = -5 V |
The 1 µm FET carried the higher drain current density and transconductance. It also had the lower normalized on-resistance. The 5 µm FET had the more negative threshold, which allowed it to serve as the driver. The on/off ratios above 10^10 supported the inverter’s low static current. BaF2 dielectric and channel-length control provided the threshold separation required for normally off operation.
Inverter transfer and power
Section titled “Inverter transfer and power”The measured voltage transfer curves covered VDD from -1 V to -5 V. The peak gain rose from -100 V/V at -1 V to -460 V/V at -5 V. The negative sign reflects the inversion of the output voltage. As the supply magnitude increased, the signal swing and gain magnitude increased.
Forward and reverse scans showed a hysteresis voltage of about 0.1 V. The static-power curve reached about 1 pW at VDD = -5 V. The inverter measurements also reported dynamic power of about 0.25 µW for supplies between -1 V and -5 V. The authors said these power values were 3 or 4 orders of magnitude below the earlier diamond inverter.
Ring oscillator performance
Section titled “Ring oscillator performance”Each ring oscillator cascaded inverter stages and added one inverter as an output buffer. The five-stage and seven-stage circuits were measured from VDD = -1 V to -3 V. Both produced stable electrical output signals over the stated supply range.
At -3 V, the five-stage oscillator reached 58.8 kHz and a 1.7 µs stage delay. The seven-stage oscillator reached 21.6 kHz and a 3.3 µs stage delay under the same supply. The authors calculated stage delay as τpd = 1/(2 × n × f), where n is the stage count and f is frequency. Output amplitude increased as the supply became more negative. Frequency was lower for seven stages than for five stages.
Comparison with earlier logic
Section titled “Comparison with earlier logic”An early E/D MESFET inverter reached a gain of 3.3 V/V at VDD = -10 V. A LaAlO3/Al2O3 E-mode driver with an Al2O3 depletion-mode load reached 26.1 V/V. A SiO2 depletion-mode load with an Al2O3 E-mode driver reached 36.3 V/V and operated up to 200 °C.
The new inverter’s peak gain exceeded those reported values at a supply magnitude of 5 V. The paper reports the highest gain and the lowest supply voltage among the compared diamond inverters. The static and dynamic power values were also 3 or 4 orders of magnitude below the earlier diamond inverter.
Earlier diamond logic demonstrations were inverters, while this work added five-stage and seven-stage oscillators. The oscillator results are the first experimental ring oscillators reported for diamond logic.
Limits and engineering implications
Section titled “Limits and engineering implications”The authors call the ring oscillator a proof of concept. Its output swing remained limited, which they associate with nonideal inverter characteristics and parasitic resistance and capacitance. Further device and circuit optimization is needed to improve oscillation amplitude.
All reported transistor and circuit measurements were made at room temperature. The paper does not demonstrate operation at the 200 °C reported for an earlier inverter. The demonstrated logic also uses p-channel H-diamond FETs, with no complementary n-channel circuit reported.
For device engineers, termination and interface processing belong to the electrical design. Hydrogen plasma creates the two-dimensional hole gas, Au protects it during contact fabrication, and BaF2 supports threshold control. Channel length also separates the load and driver thresholds, so transistor sizing is part of circuit design. The next targets named by the authors are larger oscillation swing and reduced parasitic resistance and capacitance.
Materials and support
Section titled “Materials and support”The paper needs an MPCVD-grown single-crystal diamond active layer with hydrogen termination and Au contacts for Al/BaF2-gated p-channel logic. 6CCVD’s diamond materials catalog lists MPCVD-grown single-crystal diamond and Au metallization. Its engineering support service can address the custom termination, BaF2/Al gate, and Al interconnection requirements.
View Original Abstract
Hydrogen-terminated diamond field effect transistors (FETs) are typically depletion-mode devices, which limits their application in low-power-consumption logic circuits. Here, high-performance inverters and ring oscillators have been demonstrated by using normally-off Al/BaF2/H-diamond FETs. The adoption of enhancement-mode transistors enables the realization of low-static-power logic circuits by employing diamond FETs with different channel lengths as load and driver devices. The peak gain of the inverter increases from −100 V/V to −460 V/V as the supply voltage ranges from −1 V to −5 V with a static power consumption low to ~1 pW, marking the highest gain reported for diamond-based inverters. Furthermore, a five-stage ring oscillator operates at 58.8 kHz with a stage delay of 1.7 μs under a supply voltage of −3 V, marking the first successful implementation of a diamond-based ring oscillator. These results highlight the great potential of diamond technology for high-speed power integrated circuit applications.
Electronic Grade Intrinsic Diamond Epitaxial Wafer H Terminated Superior 100 Mosfet Ready Substrate