Skip to content

Emergence of superconductivity in Th3P4-type Sn3Se4 and Ge3S4 under high pressure synthesized by diamond anvil cell with boron-doped diamond electrodes

FieldValue
JournalFigshare
Published2026-07-23
AuthorsRyo Matsumoto, Satoshi Nakano, Kensei Terashima, Toru Shinmei, Tetsuo Irifune
DOI10.6084/m9.figshare.33071740

Ge₃S₄ produced the highest onset transition temperature in the reported dataset: 10.4 K at 11 GPa. Sn₃Se₄ reached 7.9 K at 8 GPa. The largest zero-temperature upper critical field was 12.4 T for Ge₃S₄ at 11 GPa.

Pressure-dependent transition temperatures

Section titled “Pressure-dependent transition temperatures”

The authors measured temperature-dependent electrical resistance under high pressure. They evaluated transitions with onset, middle, and zero criteria. Table S1 reports the onset temperatures and zero-temperature upper critical fields.

MaterialPressure (GPa)Tc onset (K)μ₀Hc₂(0) (T)
Sn₃Se₄234.31.8
Sn₃Se₄194.9Not reported
Sn₃Se₄156.12.6
Sn₃Se₄127.14.1
Sn₃Se₄87.94.4
Ge₃S₄306.84.7
Ge₃S₄277.85.1
Ge₃S₄228.55.6
Ge₃S₄169.97.6
Ge₃S₄1110.412.4

Within each compound’s sampled range, the onset transition rose as pressure fell. Sn₃Se₄ changed from 4.3 K at 23 GPa to 7.9 K at 8 GPa. Ge₃S₄ changed from 6.8 K at 30 GPa to 10.4 K at 11 GPa.

Each series reaches its highest reported onset temperature at its lowest listed pressure. The two lists contain no common pressure point, so they do not support a direct comparison at the same pressure.

The onset table also stops at 8 GPa for Sn₃Se₄ and 11 GPa for Ge₃S₄. It does not describe resistance below those measurement points. The measured trend shows pressure dependence over the sampled high-pressure interval. The supplied material does not identify the mechanism behind that trend.

High-pressure synthesis and phase analysis

Section titled “High-pressure synthesis and phase analysis”

Both target compounds were synthesized at high pressure in a diamond anvil cell fitted with boron-doped diamond electrodes. Figure S1 shows typical LeBail refinement results for Sn₃Se₄ and Ge₃S₄ after synthesis. Figure S2 follows the ratio of peak intensities for each phase during Sn₃Se₄ synthesis.

Those figures document the refinement and phase-tracking procedures used during the study. The supplied text gives no numerical phase ratios or phase fractions. It also omits the synthesis temperature and dwell time.

The structural result therefore rests on LeBail-refined patterns, while phase proportions remain unquantified in the supplied material. The pressure-dependent peak-intensity series is presented for Sn₃Se₄ only. A comparable phase-ratio series for Ge₃S₄ is not included in the supplemental text.

Pressure was calibrated using a ruby peak for Sn₃Se₄ and the Raman peak of diamond for Ge₃S₄. Table S2 lists the stroke, optical peak, and assigned pressure for each calibration point.

MaterialPressure referenceStroke (μm)Peak position (nm)Pressure (GPa)
Sn₃Se₄Ruby0702.523
Sn₃Se₄Ruby−40701.2519
Sn₃Se₄Ruby−60699.715
Sn₃Se₄Ruby−70698.612
Sn₃Se₄Ruby−80697.18
Sn₃Se₄Ruby−90695.94
Ge₃S₄Diamond Raman0139930
Ge₃S₄Diamond Raman−40139427
Ge₃S₄Diamond Raman−50138222
Ge₃S₄Diamond Raman−60136916
Ge₃S₄Diamond Raman−70135911

For Sn₃Se₄, the ruby peak was 695.9 nm at 4 GPa and 702.5 nm at 23 GPa. The stroke changed from −90 to 0 μm over that interval. For Ge₃S₄, the diamond Raman peak was 1359 nm at 11 GPa and 1399 nm at 30 GPa. Its stroke changed from −70 to 0 μm.

Both optical references shifted to longer wavelengths at higher assigned pressure. The two runs used different reference signals and different stroke sets. Table S2 lists no calibration uncertainty and no shared calibration point. The pressure assignments span 4 to 30 GPa across the two materials.

The reported zero-temperature upper critical field increased toward lower pressure in both series. At 30, 27, 22, and 16 GPa, Ge₃S₄ had fields of 4.7, 5.1, 5.6, and 7.6 T. At 11 GPa, its field reached 12.4 T.

Sn₃Se₄ had reported fields of 1.8 T at 23 GPa, 2.6 T at 15 GPa, 4.1 T at 12 GPa, and 4.4 T at 8 GPa. The 19 GPa value is not reported.

Even the lowest listed Ge₃S₄ field, 4.7 T at 30 GPa, exceeds the highest listed Sn₃Se₄ field, 4.4 T at 8 GPa. That comparison does not remove the pressure mismatch between the series.

Figure S6 shows the temperature dependence of μ₀Hc₂ at several pressures. The supplied text gives no fitting function or uncertainty for μ₀Hc₂(0). No prior-work upper critical fields are listed for either compound. The field comparison is therefore confined to the pressure points reported within each material.

Figure S3 sets out the determination method for Tc onset, Tc middle, and Tc zero. Its caption does not reproduce the numerical thresholds used for those criteria.

Figure S4 compares the pressure dependence of Tc under each criterion and shows the transition width, defined as Tc onset minus Tc zero. The supplied text gives no numerical transition widths. Table S1 uses the onset criterion throughout, so its listed temperatures can be compared without mixing criteria. Zero and middle values cannot be recovered from the supplied tables.

The equation of state was fitted with a third-order Birch-Murnaghan equation. Figure S5 examines the B₀′ dependence of the fitted B₀ and V₀ parameters for Sn₃Se₄ and Ge₃S₄.

No numerical B₀, V₀, or B₀′ outputs appear in the supplied text. The material therefore supports the stated fitting approach but not a quantitative comparison of the fitted bulk parameters. These figures document the analysis method, while numerical verification depends on reading the plotted results.

Implications for pressure-cell material selection

Section titled “Implications for pressure-cell material selection”

The direct material requirement is boron-doped diamond for the diamond anvil cell electrodes. The authors combine high-pressure synthesis with electrical resistance measurements under pressure. Reproducing the work therefore requires the electrode-equipped cell to operate at the reported pressures.

The supplied material contains no comparison of boron-doped diamond electrodes with another electrode material. It does not establish performance superiority. Electrode dimensions, boron concentration, contact resistivity, temperature limit, and cycle life are also absent. These omissions prevent an electrode specification based on measured interface performance or lifetime.

Do not treat 10.4 K or 7.9 K as zero-resistance operating temperatures. The study distinguishes onset, middle, and zero criteria, and Table S1 provides only onset values. For material selection, the onset temperature compares transition behavior within the reported series. The upper critical field reports the field scale at each pressure point.

Before adopting either compound or its electrode material in a design, obtain the raw resistance curves, zero and middle transition temperatures, field uncertainties, phase ratios, and equation-of-state outputs. Without those records, the study documents boron-doped diamond electrodes and high-pressure transition points. It does not provide full device qualification.

6CCVD’s diamond materials catalog lists boron-doped diamond, the electrode material named for this diamond anvil cell synthesis. The application requires boron-doped diamond electrodes for high-pressure synthesis, and engineering support can be used to discuss that electrode material requirement.

View Original Abstract

High-pressure techniques provide a powerful approach for exploring superconducting materials by enabling structural modifications that significantly alter electronic and phonon properties. In this study, we investigate the emergence of superconductivity in Sn<sub>3</sub>Se<sub>4</sub> and Ge<sub>3</sub>S<sub>4</sub> with the Th<sub>3</sub>P<sub>4</sub>-type cubic structure using high-pressure synthesis and in situ electrical transport measurements in a diamond anvil cell equipped with boron-doped diamond electrodes. Both compounds exhibit superconductivity, with maximum transition temperature <i>T</i><sub>c</sub> of 7.9 K at 8 GPa for Sn<sub>3</sub>Se<sub>4</sub> and 10.5 K at 11 GPa for Ge<sub>3</sub>S<sub>4</sub>. The behavior of the <i>T</i><sub>c</sub> as a function of pressure and previously reported theoretical calculations, including related compounds, suggest a phonon-mediated BCS-type mechanism for observed superconductivity. These results expand the family of Th<sub>3</sub>P<sub>4</sub>-type superconductors and demonstrate the effectiveness of high-pressure techniques for discovering new superconducting phases. Sn<sub>3</sub>Se<sub>4</sub> and Ge<sub>3</sub>S<sub>4</sub> are synthesized at high pressure, and superconductivity in both compounds has been reported for the first time.