Construction optimization and functional applications of fluorescent nanodiamonds

FieldValue
JournalResponsive materials
Published2026-09-23
AuthorsYunpeng Yang, Sen Zhang, Chao Chen, Wensi Yang, Zuanquan Chen
DOI10.1002/rpm2.70081
Citations1

Fluorescent nanodiamonds now support quantum emitters, biological sensors, and integrated photonic devices. The review reports a 7,800-fold sensitivity gain over colloidal gold in a saliva assay based on NV spin control. One cited fabrication process produced 250 g/day and more than 1 kg/week of roughly 50 nm particles.

Fluorescent nanodiamonds range from several nanometers to hundreds of nanometers and contain optically active lattice defects. Intrinsic diamond has a 5.5 eV band gap. The review describes more than 100 impurity or vacancy color centers with ultraviolet to near-infrared emission.

The negatively charged NV center has a spin-triplet ground state with a zero-field splitting of about 2.87 GHz. Its excited state has a splitting of about 1.42 GHz. The 637 nm zero-phonon line is accompanied by a 500 to 800 nm photon sideband. NV centers support millisecond-scale spin coherence at room temperature, but only NV- has the spin-triplet ground state required for coherent spin manipulation.

The SiV- center has a 738 nm zero-phonon line, a spin-doublet ground state, and a g factor of about 2.002. It has no zero-field splitting and couples weakly to phonons. These properties suit single-photon sources and optical resonators.

Synthesis routes set particle size and defect quality

Section titled “Synthesis routes set particle size and defect quality”

Conventional preparation starts with diamond particles. Electron or ion irradiation creates lattice vacancies. High-temperature annealing then lets nitrogen or silicon atoms capture those vacancies. The review compares four representative routes.

RouteDemonstrated centersRepresentative sizeMain strengthMain limitation
DetonationNV, SiV, SnV4 to 20 nmGram-scale yield, low cost, intrinsic dopingGraphitic impurities, irregular agglomeration, poor center homogeneity
HPHTNV, SiV10 to 200 nmHigh monocrystalline quality, adjustable size, long spin coherencePost-irradiation, annealing, and high equipment cost
CVDSiV, NV, GeV10 to 75 nmLow sp² contamination, single-crystal particles, high-quality centersLow yield, expensive vacuum system, poor scalability
PTQNVAbout 50 nmOne-step nitrogen doping, high sp³ content, scalable productionNarrow size range and limited center types

Detonation synthesis produced particles around 10 nm. One tin-doped sample contained approximately 5 nm particles, verified by TEM and an SnV- zero-phonon line after acid purification. A silicon-doped sample averaged about 11 nm and showed NV- and SiV- lines at 637 and 738 nm.

One HPHT study used TEOS-doped carbon aerogel under laser heating at 20 to 25 GPa and 1800 to 3000 K. It produced 1 to 200 nm particles with NV and SiV- photoluminescence lines. CVD produced 10 to 75 nm SiV nanodiamonds on a vertical silicon substrate. Raman spectroscopy identified the sp³ diamond peak at 1332 cm⁻¹. A room-temperature lifetime of 0.602 ± 0.008 ns showed quenching from the substrate.

The NaCl-assisted PTQ process used 7 GPa and 1700 °C to form roughly 50 nm particles in 4 minutes. It reached 250 g/day and over 1 kg/week, about 2000-fold more efficient than traditional methods. Raman data showed 93.0% sp³ carbon. The particles had about five times the Rabi contrast of commercial material and a T1 near 1 ms.

Surface chemistry controls charge and coherence

Section titled “Surface chemistry controls charge and coherence”

Surface terminations change electron affinity, charge distribution, nonradiative recombination, and biological interactions. Oxygen-containing terminations stabilized NV-. Carboxylated particles combined with PEG linkers reduced spin noise. One neurotensin-conjugated PEG-maleimide probe recognized neurotensin receptor 1 on live-cell membranes.

A roughly 5 nm HPG coating gave FNDs more than 2 hours of colloidal stability in PBS. It increased avidin binding efficiency 83-fold. After conjugation to a mitochondrial localization signal, ODMR measured intramitochondrial temperature with less than 1 K precision.

Air oxidation at 565 °C followed by acid treatment increased T1 from about 320 µs to 470 to 490 µs. An 11 nm silica shell then raised T1 to 1.00 ± 0.06 ms, near the bulk-diamond range. Monte Carlo modeling indicated that a shell near 1 nm better balanced noise suppression and gadobutrol sensing sensitivity. Room-temperature visible-light hydrogen-atom transfer also formed C-F, C-Cl, C-S, and C-N surface bonds with little loss of coherence for NV centers within 10 nm of the surface.

Nanophotonic structures improve emission collection

Section titled “Nanophotonic structures improve emission collection”

At 4 K, a SiV nanodiamond in a hemispherical Fabry-Pérot cavity produced a Rabi frequency of 330 MHz and g²(0) = 0.33. Its excitation linewidth was about 340 MHz, while the peak moved by less than 24 MHz over 90 seconds. All-optical initialization and readout worked at fields up to 3.2 T, with 67 ns initialization, 80% fidelity, and a 350 ns spin lifetime.

A tunable fiber Fabry-Pérot cavity operated at room temperature. It reached a Purcell factor of 2 and a single-photon count rate of 1.6 × 10⁶ s⁻¹. Fluorescence was 3.8 times the free-space collection level. A back-illuminated bullseye antenna collected about 70% of forward emission at a numerical aperture of 0.5. An earlier grating antenna had a theoretical 85% collection efficiency under a 0.9 numerical aperture.

A tapered fiber and silver nanowire reached a Purcell factor of 58.6. Waveguide coupling was 5.3 times free-space collection, and the combined figure of merit exceeded 3000. A separate tapered-fiber magnetic probe achieved 80 µT/√Hz sensitivity with about 1 µm spatial resolution.

Biomedical uses exploit spin readout and targeting

Section titled “Biomedical uses exploit spin readout and targeting”

Biomedical performance depends on particle size, crystal quality, defect density, surface chemistry, and NV charge-state stability. The review reports six-dimensional tracking of single nanodiamonds on live-cell membranes. AFM-coupled ODMR also measured rotation during indentation of live cells and separated local from nonlocal deformation.

A spin-enhanced lateral-flow assay reduced the SARS-CoV-2 antigen detection limit by about three orders of magnitude versus gold-nanoparticle strips. In 103 blinded swab specimens, sensitivity was 95.1% for Ct ≤ 30 and specificity was 100%. Modelling estimated diagnosis 2.0 days earlier than conventional lateral-flow assays. It also predicted 2.2-fold more positive cases on the first day of symptoms.

A tuberculosis assay reached an ESAT-6 detection limit of 0.02 ng mL⁻¹. Testing 50 clinical samples produced 98% diagnostic accuracy and 100% discrimination between tuberculosis and nontuberculous mycobacterial infections. The mBBQ point-of-care system detected single proteins in human saliva. Its UnetConvLSTM-Attention model processed spin-dependent fluorescence signals and produced the reported 7,800-fold gain over colloidal gold.

Covalently linked FND-diazoxide probes supported sustained drug release over 72 hours. NV T2 readout tracked intracellular free radicals during release.

Limits require application-specific material selection

Section titled “Limits require application-specific material selection”

No route controls particle size, center density, crystal quality, and production efficiency at once. Detonation offers scale and low cost, but graphitic impurities and irregular agglomeration reduce center homogeneity. CVD provides low sp² contamination and single-crystal particles, but its low yield and expensive vacuum system restrict scale. HPHT offers high monocrystalline quality, while post-irradiation, annealing, and equipment cost complicate batch production.

Defect control remains the central synthesis problem. More nitrogen can raise NV generation, but excess nitrogen defects add magnetic noise and accelerate spin relaxation. The large surface-to-volume ratio also leaves shallow centers sensitive to dangling bonds, adsorbed molecules, and fluctuating charges.

For biomedical translation, protein adsorption changes corona formation, uptake, and targeting. Long-term retention, immune response, and accumulation in reticuloendothelial organs remain insufficiently characterized. Standard pharmacokinetic and toxicological protocols are still needed.

Material selection should therefore follow the application. NV magnetometry needs stable termination, long T1, controlled defect density, and efficient collection. SiV photonics needs narrow linewidth, controlled placement, cavity coupling, and high extraction. Biological probes need a defined size distribution, colloidal stability, targeting ligands, and evidence of long-term safety. These properties must be specified together because improving one can degrade another.

For nanophotonic integration, the paper patterns designer nanodiamonds on single-crystal diamond substrates and transfers them to thin-film silicon nitride for coupling with waveguides and microring resonators. 6CCVD’s diamond materials catalog lists MPCVD-grown single-crystal diamond plates and wafers up to 125 mm, with thickness from 0.1 to 500 µm. Engineering support can help define custom substrate and fabrication requirements for the integrated device.

View Original Abstract

Abstract Fluorescent nanodiamonds (FNDs) have emerged as a versatile and powerful quantum platform across quantum technologies, biomedical sciences, and industrial sensing, owing to their exceptional optical properties, excellent spin coherence, inherent biocompatibility, and remarkable environmental robustness. In recent years, notable advances have been achieved covering both well‐established and newly discovered diamond color centers, the controllable fabrication of high‐quality FNDs, the integration with nanophotonic devices, and the expansion of application scenarios. This review provides a comprehensive and critical overview of the latest research advances in FNDs, focusing on the development of novel color‐center species, advanced synthetic and surface‐modification strategies, nanophotonic integration technologies, and cutting‐edge applications in quantum sensing, single‐photon emission, and biomedicine. We further present a critical assessment of current challenges and an insightful outlook on future trends. This review aims to offer a unified perspective for interdisciplinary researchers and promote the practical translation and advanced developments of FND‐based technologies.