Simulated three-dimensional boron-doped diamond anode applied to the treatment of organic-polluted wastewater with simultaneous hydrogen production
Paper details
Section titled “Paper details”| Field | Value |
|---|---|
| Journal | Journal of environmental chemical engineering |
| Published | 2026-11-01 |
| Authors | Gabriel Palace, Ricardo Sgarbi, Luisa G. Franco, Luís A.M. Ruotolo |
| DOI | 10.1016/j.jece.2026.125804 |
Three parallel mesh-type boron-doped diamond anodes produced the fastest total organic carbon (TOC) mineralization in real herbicide wastewater. Their apparent rate constant was 0.08445 min⁻¹, against 0.05145 min⁻¹ for the stacked three-dimensional anode and 0.02815 min⁻¹ for one mesh anode. The comparison used 60 mA cm⁻², 0.15 m s⁻¹, and 55 °C. Hydrogen evolution retained near-unity Faradaic efficiency across the tested organic matrices.
Architecture and operating conditions
Section titled “Architecture and operating conditions”Three overlapping commercial mesh-type BDD electrodes simulated a porous three-dimensional anode, designated 3DS-BDD. Each mesh measured 5 cm × 10 cm × 0.15 cm, and one mesh, called M-BDD, served as the reference. The authors later proposed three independent mesh electrodes in parallel, called 3M-BDD, to avoid the flow restriction of the stack.
The semi-pilot flow cell used polyacetal, a nickel mesh cathode, plastic mesh turbulence promoters, and an AMI-7001S anion exchange membrane. The anolyte was 0.1 M Na2SO4, and the catholyte was 3.0 M KOH. Each BDD electrode was cleaned at 0.2 A for 10 min in 0.1 M Na2SO4.
Cyclic voltammetry with ferricyanide and ferrocyanide gave the electroactive area through the Randles-Sevcik relation. Limiting currents at 0.05 to 0.31 m s⁻¹, equal to 1 to 6 L min⁻¹, gave the mass-transfer parameters. A movable Ag/AgCl reference measured potential through the 4.5 mm electrode thickness.
TOC was measured with a Sievers InnovOx 900, while COD used Hach digestion vials and the potassium dichromate colorimetric method.
Active area and intrinsic transport diverged
Section titled “Active area and intrinsic transport diverged”The electroactive area was 41.6 cm² for M-BDD and 107 cm² for 3DS-BDD. Their ratio was 2.57, below the threefold value expected from three identical meshes. This indicates that some stacked area became less electrochemically active.
Potential measurements showed more positive potentials near the current feeder and lower potentials downstream. The gradient grew with distance from the electrical contact. The authors therefore linked the higher mass-transfer product of 3DS-BDD to added area, not a higher intrinsic mass-transfer coefficient. M-BDD retained the higher coefficient.
The proposed mechanism was reduced void space in the stack and preferential flow through the more open turbulence promoter. The authors called for experimental or computational fluid dynamics evidence.
M-BDD with turbulence promoters produced higher Sherwood numbers over the tested Reynolds range. Its performance was comparable to or better than several reported flat-plate, filter-press, and reticulated vitreous carbon reactors. At 0.15 m s⁻¹, Re was 1886 and Sh was 1267. Raising velocity from 0.15 to 0.21 m s⁻¹ increased the mass-transfer coefficient by 8.8%, less than the 16% gain from 0.10 to 0.15 m s⁻¹.
Hydrogen production separated charge conversion from energy efficiency
Section titled “Hydrogen production separated charge conversion from energy efficiency”The cathodic reaction produced hydrogen at a constant rate, with linear fits having R² > 0.99. Hydrogen volume was measured by displacement of a sealed water-filled column. Faradaic efficiency was close to 100% in every hydrogen-production assay.
Energy efficiency was much lower, ranging from 13% to 28%. The maximum used a 50 cm² projected cathode, 4 A, 80 mA cm⁻², and 0.15 m s⁻¹. Its cell voltage was 10.4 ± 0.4 V. A 10 cm² cathode at 3 A and 0.15 m s⁻¹ gave the lowest cell voltage, 8.0 ± 0.6 V.
Higher flow did not lower cell voltage consistently. The authors suggest that the tested range did not remove bubbles effectively. Another possibility was that faster flow dispersed more gas and increased resistance in the liquid electrolyte.
Pollutant structure controlled mineralization kinetics
Section titled “Pollutant structure controlled mineralization kinetics”Phenol, aniline, glyphosate, formic acid, oxalic acid, and maleic acid were tested separately at 300 mg L⁻¹. Mixtures retained the same total concentration. TOC and COD were measured during electrolysis. Both decays followed pseudo-first-order kinetics, with R² values of at least 0.96.
Phenol and aniline mineralized more slowly than the carboxylic acids. In the 30 mA cm⁻² test at 0.15 m s⁻¹, about 20% to 25% of initial TOC remained after 60 min. At 60 mA cm⁻² and 0.15 m s⁻¹, the TOC rate constant was 4.00 × 10⁻³ s⁻¹ for phenol and 3.50 × 10⁻³ s⁻¹ for aniline. The three carboxylic acids ranged from 8.50 × 10⁻³ to 10.5 × 10⁻³ s⁻¹.
COD profiles were nearly independent of molecular structure. Their similar decay and comparable mass-transfer coefficients support mass-transfer control of oxidation. TOC mineralization depended on molecular structure and oxidation pathway. The authors attribute slower aromatic removal to the energy needed to cleave the ring.
Global energy consumption was 148 kWh kg⁻¹ for phenol and 154 kWh kg⁻¹ for aniline. Maleic acid required 98 kWh kg⁻¹, while formic acid required 129 kWh kg⁻¹. The glyphosate plus phenol mixture had the highest value, 182 kWh kg⁻¹.
Hydrogen rate constants ranged from 9.94 × 10⁻⁵ to 11.64 × 10⁻⁵ m³ s⁻¹ m⁻² across the model electrolytes. Their fits had R² ≥ 0.98, and the rates did not change materially with anolyte composition.
Parallel meshes gave the fastest mineralization
Section titled “Parallel meshes gave the fastest mineralization”Real wastewater came from triple washing of glyphosate and tebuthiuron containers. The source wastewaters had typical COD of 100 to 300 mg L⁻¹. Tests used TOC of 45 mg L⁻¹ and COD of 180 mg L⁻¹. The current was 60 mA cm⁻², flow was 0.15 m s⁻¹, and temperature was 55 °C. Supporting electrolyte was added because the industrial washwater had low conductivity.
| Configuration | Mass-transfer coefficient (m s⁻¹) | TOC rate constant (min⁻¹) | Global current efficiency (%) | Global energy use (kWh kg⁻¹ TOC) |
|---|---|---|---|---|
| M-BDD | 3.67 × 10⁻⁵ | 0.02815 | 10.3 | 408 |
| 3DS-BDD | 1.43 × 10⁻⁵ | 0.05145 | 13.4 | 234 |
| 3M-BDD | Not reported | 0.08445 | Not shown | 408 |
At the same nominal current density, effective current density was 72 mA cm⁻² for M-BDD and 28 mA cm⁻² for 3DS-BDD. This lower effective loading supported the higher current efficiency of the stacked anode.
The 3M-BDD current efficiency was essentially the same as M-BDD and was not plotted. It reached normalized TOC of about 0.08 in 30 min. The stack required 50 min for the same conversion.
The stack therefore offered lower energy use, while the parallel assembly offered faster treatment and lower required anode area. The 3M-BDD configuration also avoided the stacked assembly’s internal potential gradient.
Limits for scale-up
Section titled “Limits for scale-up”Cell voltage remained the main hydrogen energy penalty. Near-complete charge conversion therefore did not produce low specific energy use.
Complete mineralization became less efficient as TOC fell. The authors used 10 mg L⁻¹ as the endpoint for global calculations. They note that adsorption may then be more effective and economical for finishing treatment.
The study operated at semi-pilot scale and used container washwater with added supporting electrolyte. It did not report performance without supporting electrolyte for this low-conductivity stream. Plant-scale fabrication and cost assessment were also absent.
The authors expect pressure drop to rise with the square of flow velocity. Higher velocity therefore increases pumping demand as mass-transfer gains become smaller. They also treat BDD purchase cost as a constraint, making effective use of the purchased area a central design criterion.
Materials and support
Section titled “Materials and support”The paper applies boron-doped diamond to organic oxidation in a wastewater electrolyzer that also produces hydrogen and requires mesh anodes in 0.1 M Na2SO4. The diamond materials catalog includes boron-doped diamond, matching the required anode material family, although it does not specify the paper’s mesh form. For the modular reactor, 6CCVD’s engineering support covers the custom fabrication required for the parallel-mesh assembly.
View Original Abstract
Three-dimensional (3D) electrode architectures have emerged as a promising strategy to improve the electrochemical treatment of wastewater, since they offer an increased electroactive area ( A e ) and enhanced mass transfer. However, the interplay among A e , mass transfer, and electrode potential distribution in three-dimensional electrodes remains poorly understood. This work investigated these effects using aromatic compounds, carboxylic acids, herbicides, multicomponent electrolytes, and real wastewaters, under different hydrodynamic conditions. A simulated three-dimensional boron-doped diamond (BDD) anode (3DS-BDD), assembled by stacking commercial mesh-BDD (M-BDD) electrodes, was developed to distinguish the contributions of A e and mass transfer coefficients ( k m ). Cyclic voltammetry showed that A e increased from 41.6 to 107 cm 2 , while Sherwood-Reynolds correlations revealed modified transport behavior. Although 3DS-BDD exhibited higher apparent mass transfer parameters ( k m A ), the corresponding k m values were lower than for the M-BDD electrode. Electrode potential measurements revealed a non-uniform distribution, demonstrating that the increase in k m A originated from the enlarged area, rather than intrinsic mass transfer enhancement. Electrooxidation followed pseudo-first order kinetics, while hydrogen evolution proceeded with near-unity Faradaic efficiency, irrespective of the wastewater composition. Comparable k m values for all the organic matrices indicated that mass transfer governed by reactor hydrodynamics, rather than pollutant properties. The results showed that the most efficient reactors should combine enlarged A e with higher k m . The proposed modular 3M-BDD concept addresses these requirements by preserving the favorable hydrodynamics of individual mesh electrodes, while providing a large A e , offering a promising strategy for the scale-up of electrochemical wastewater treatment integrated with low-carbon hydrogen production.
Boron Doped Diamond On Titanium Bdd Electrode
View Specs →
Boron Doped Diamond Electrode On Niobium Bdd Nb Electrode
View Specs →