Anodic Oxidation of Aqueous Wastes Containing Hydroquinone on BDD Electrode
At a Glance
Section titled āAt a Glanceā| Metadata | Details |
|---|---|
| Publication Date | 2015-01-01 |
| Journal | Journal of Advanced Oxidation Technologies |
| Authors | H. Trabelsi, Nasr Bensalah, Abdellatif Gadri |
| Institutions | Texas A&M University at Qatar, University of Sfax |
| Citations | 9 |
Abstract
Section titled āAbstractāAbstract The electrochemical oxidation of 1,4 dihydroxybenzene, was studied by galvanostatic electrolysis using boron-doped diamond (BDD) as anode. The efficiency of the electrochemical process was found to depend mainly on the pollutant concentration present in the waste and on the applied current density. The voltammetric results showed that hydroquinone oxidation takes place in the same potential region as that of phenol where the supporting electrolyte is stable. Synthetic wastewaters containing hydroquinone have been treated in a bench-scale electrolysis plant. This plant operates in a discontinuous mode by recirculating the waste continuously through a single-chamber electrochemical flow cell. The complete mineralization of hydroquinone and the electro-generated pollutants is obtained in the electrolytic device. HPLC analyses show the formation of carboxylic acids as the main intermediates. The high efficiency of this technology can be explained in terms of the direct electro-oxidation at the BDD surface and the oxidation carried out by hydroxyl radicals and other electro-generated oxidants.