The Effect of h-BN Additive on the Structure of Diamond Crystal
At a Glance
Section titled āAt a Glanceā| Metadata | Details |
|---|---|
| Publication Date | 2015-01-01 |
| Journal | Journal of Changchun University of Science and Technology |
| Authors | LI Peihan |
| Institutions | Materials Science & Engineering, Changchun University of Science and Technology |
Abstract
Section titled āAbstractāIn this work,we report the growth process of single crystal diamond by doping boron(B) and hexagonal boron nitride(h-BN) in the system of Fe70Ni30 alloy catalyst and graphite. The doping of B and h-BN has significant effect on the growth condition and morphology of diamonds. The lowest growth pressure of h-BN doped diamond is 6.2Gpa and the crystals have a green strip morphology. This results indicates that B and h-BN have different effects on the diamond growth and have different ways to replace carbon atoms. We analyze the effect of doping B and N atoms on the structure of diamond,and the chemical environment of B and N atoms in diamond by using X-ray diffraction and photoelectron spectroscopy. The mechanism of B and N doped diamond is also demonstrated.
Tech Support
Section titled āTech SupportāOriginal Source
Section titled āOriginal Sourceā- DOI: None