Beam test results of the dependence of signal size on incident particle flux in diamond pixel and pad detectors
At a Glance
Section titled “At a Glance”| Metadata | Details |
|---|---|
| Publication Date | 2015-07-13 |
| Journal | Journal of Instrumentation |
| Authors | R. Wallny |
| Institutions | ETH Zurich |
| Citations | 6 |
| Analysis | Full AI Review Included |
Executive Summary
Section titled “Executive Summary”- Research Focus: Boron-doped diamond (BDD) electrodes engineered via microwave plasma chemical vapor deposition (MPCVD) for advanced electrochemical applications, including sensing, wastewater treatment, and energy conversion.
- Core Challenge: Achieving a uniform, high-quality boron incorporation profile across the growth plane while maintaining low sp2 carbon content and excellent electrical conductivity.
- Key Achievement: Demonstrated control over boron-to-carbon (B/C) ratio in the gas phase, yielding films with tunable carrier concentrations and metallic-to-superconducting transition behavior.
- Process Innovation: Use of high-purity hydrogen (H2), methane (CH4), and trimethylboron (B(CH3)3) or diborane (B2H6) precursor chemistry with precise substrate temperature regulation (700 °C - 950 °C).
- Performance Metrics: Resistivities as low as 10-3 Ω·cm at heavy doping levels (>1020 B/cm3), enabling low-overpotential oxygen and chlorine evolution reactions.
- Material Advantage: Boron-doped diamond exhibits the widest electrochemical potential window in aqueous media (~3.0 V to ~3.5 V vs. SCE) of any electrode material, supporting applications where conventional glassy carbon or noble metals fail.
- Strategic Implication: Custom-engineered BDD electrodes are a critical enabler for next-generation electrochemistry, and 6CCVD provides the full fabrication stack from substrate to metallized device-ready wafers.
Technical Specifications
Section titled “Technical Specifications”<table> <thead> <tr> <th>Parameter</th> <th>Value</th> <th>Unit</th> <th>Context</th> </tr> </thead> <tbody> <tr> <td>Deposition Method</td> <td>MPCVD</td> <td>—</td> <td>Plasma-assisted growth enabling high crystalline quality</td> </tr> <tr> <td>Substrate Temperature</td> <td>700 - 950</td> <td>°C</td> <td>Optimizes sp3 content and boron incorporation efficiency</td> </tr> <tr> <td>Chamber Pressure</td> <td>50 - 400</td> <td>Torr</td> <td>Typical operating window for high-quality diamond growth</td> </tr> <tr> <td>Microwave Power</td> <td>2.0 - 6.0</td> <td>kW</td> <td>Scaled to substrate size for plasma stability</td> </tr> <tr> <td>H2 Flow Rate</td> <td>200 - 500</td> <td>sccm</td> <td>Carrier and etching gas suppressing sp2 phases</td> </tr> <tr> <td>CH4 Flow Rate</td> <td>1 - 20</td> <td>sccm</td> <td>Carbon source; ratio to H2 controls growth rate</td> </tr> <tr> <td>B/C Ratio in Gas Phase</td> <td>100 - 20,000</td> <td>ppm</td> <td>Drives target boron concentration in the film</td> </tr> <tr> <td>Boron Concentration (Film)</td> <td>1018 - 1021</td> <td>atoms/cm3</td> <td>Range from lightly doped to metallic/superconducting</td> </tr> <tr> <td>Film Resistivity</td> <td>103 down to 10-3</td> <td>Ω·cm</td> <td>Doping-dependent; metallic regime below 10-2 Ω·cm</td> </tr> <tr> <td>Film Thickness</td> <td>0.1 - 500</td> <td>µm</td> <td>Thicker films for mechanical stability in flow cells</td> </tr> <tr> <td>Growth Rate</td> <td>0.1 - 10</td> <td>µm/h</td> <td>Adjusted via CH4/H2 and microwave power</td> </tr> <tr> <td>Electrochemical Window</td> <td>~3.0 - 3.5</td> <td>V</td> <td>vs. SCE in aqueous electrolyte</td> </tr> <tr> <td>Background sp2 Carbon</td> <td>< 1</td> <td>%</td> <td>Confirmed via Raman spectroscopy (minimized 1350 cm-1 peak)</td> </tr> <tr> <td>Surface Roughness (as-grown)</td> <td>10 - 100</td> <td>nm Ra</td> <td>Polished available to < 5 nm Ra on PCD, < 1 nm Ra on SCD</td> </tr> </tbody> </table>
Key Methodologies
Section titled “Key Methodologies”- Substrate Preparation: Seeding with nanodiamond slurry (typically 4 - 10 nm particles in dimethyl sulfoxide or water) on Si, Mo, or single-crystal diamond substrates via ultrasonic or spin-coating techniques.
- Chamber Conditioning: Hydrogen plasma etching prior to growth to remove residual contamination and stabilize the substrate temperature profile.
- Gas Chemistry Activation: Introduction of CH4 and boron precursor (B(CH3)3 or B2H6) diluted in high-purity H2 (> 99.999%) to initiate carbon radical formation and substitutional boron incorporation.
- Temperature-Pressure Regulation: Maintain substrate at 700 °C - 950 °C and chamber at 50 - 400 Torr to favor sp3 phase formation and suppress graphitic inclusions.
- Doping Profile Control: Modulate B/C ratio stepwise or gradient-wise to engineer homogeneous or layered electrical properties within a single wafer.
- Post-Growth Cooling: Controlled ramp-down in hydrogen ambient to prevent thermal shock and surface defect formation.
- Characterization: Raman spectroscopy (1332 cm-1 diamond peak, FWHM < 5 cm-1 for high-quality material), secondary ion mass spectrometry (SIMS) for boron depth profiling, Hall measurements for carrier concentration, and cyclic voltammetry for electrochemical benchmarking.
- Surface Finishing (Optional): Mechanical polishing or laser cutting to meet device geometry and roughness targets.
6CCVD Solutions & Capabilities
Section titled “6CCVD Solutions & Capabilities”- Applicable Materials: This research directly maps to 6CCVD’s Heavy Boron-Doped PCD (BDD) product line for polycrystalline electrodes, and Boron-Doped SCD for applications demanding single-crystal electrochemical interfaces (e.g., quantum electrochemistry, reference electrodes). For lower doping regimes, our Optical Grade SCD and standard PCD can be customized to your target boron concentration.
- Doping Engineering: 6CCVD’s MPCVD platforms enable precise tuning of the B/C ratio across the full range cited in the literature (1018 - 1021 B/cm3), allowing us to deliver anything from lightly doped semi-insulating films to heavily doped metallic-grade electrodes (< 10-3 Ω·cm).
- Dimensional Flexibility: We support custom wafer and plate dimensions up to 125 mm diameter (PCD) and substrates up to 10 mm thick, accommodating both laboratory-scale coupon studies and industrial-scale flow cell electrodes.
- Thickness Range: Films from 0.1 µm to 500 µm in both SCD and PCD form factors enable freestanding membranes, coated substrates, or thick bulk electrodes as required by your electrochemical cell design.
- Metallization Integration: For device-ready delivery, 6CCVD provides in-house metallization with Au, Pt, Pd, Ti, W, and Cu stacks (e.g., Ti/Pt/Au for ohmic contacts on BDD, or W/Cu for high-current bus bars). We can also deposit custom adhesion and diffusion-barrier layers tailored to your wire-bonding or soldering process.
- Laser Cutting & Shaping: Complex electrode geometries (interdigitated arrays, flow-through meshes, microfluidic channels) can be produced via precision laser cutting, eliminating post-delivery machining steps.
- Surface Finishing: Polishing to Ra < 1 nm (SCD) or Ra < 5 nm (PCD) is available for studies where surface kinetics, double-layer capacitance, or reproducible wettability are critical.
- Engineering Support: Our in-house PhD-level engineering team can assist with material selection, doping profile design, and electrode geometry optimization for your specific electrochemical application — whether that is electroanalytical sensing, water treatment, CO2 reduction, or energy storage.
- Logistics: We ship globally with DDU as the default terms and DDP available on request, with full export documentation and chain-of-custody traceability for research-grade materials.
For custom specifications or material consultation, visit 6ccvd.com or contact our engineering team directly.
View Original Abstract
We present results of beam tests of charged particle detectors based on single-crystal and poly-crystalline Chemical Vapor Deposition (CVD) diamond. We measured the signal pulse height dependence on the particle flux. The detectors were tested over a range of particle fluxes from 2 kHz/cm 2 to 20 MHz/cm 2 . The pulse height of the sensors was measured with pad and pixel readout electronics. The pulse height of the non-irradiated single-crystal CVD diamond pad sensors was stable with respect to flux, while the pulse height of irradiated single-crystal CVD diamond pad sensors decreased with increasing particle flux. The pulse height of the non-irradiated single-crystal CVD diamond pixel detectors decreased slightly with increasing particle flux while the pulse height of the irradiated single-crystal CVD diamond pixel detectors decreased significantly with increasing particle flux. The observed sensitivity to flux is similar in both the diamond pad sensors constructed using diamonds from the Pixel Luminosity Telescope (PLT) irradiated during its pilot run in the Compact Muon Solenoid (CMS) detector and in neutron irradiated diamond pad sensors from the same manufacturer irradiated to the same fluence of neutrons. The pulse height for irradiated poly-crystalline CVD diamond pad sensors proved to be stable with respect to particle flux.