Effect of Cutting Force Control on Cutting Characteristics of CFRP in Diamond Saw Cutting

MetadataDetails
Publication Date2015-07-23
JournalKey engineering materials
AuthorsYuki Doi, Yasuo Kondo, Satoshi Sakamoto, Kenji Yamaguchi
InstitutionsYamagata University Hospital, National Institute of Technology, Yonago College
Citations1

We examined the relation between the cutting force and the cutting characteristics of CFRP in diamond saw cutting. When a larger cutting force was applied, the cutting had been propagated with a mixed mechanism of the cutting by cutting edges and the cleaving of carbon fiber by shear force. While a good cutting surface was formed in the case of cutting with less than 23 N of cutting force. In this condition, the cutting had been propagated only by the cutting with cutting edges.