Influence of Fiber Orientation on Single-Point Cutting Fracture Behavior of Carbon-Fiber/Epoxy Prepreg Sheets
At a Glance
Section titled “At a Glance”| Metadata | Details |
|---|---|
| Publication Date | 2015-10-02 |
| Journal | Materials |
| Authors | Yingying Wei, Qinglong An, Xiaojiang Cai, Ming Chen, Weiwei Ming |
| Institutions | Shanghai Jiao Tong University |
| Citations | 21 |
| Analysis | Full AI Review Included |
ERROR: File too large (12.9MB)
View Original Abstract
The purpose of this article is to investigate the influences of carbon fibers on the fracture mechanism of carbon fibers both in macroscopic view and microscopic view by using single-point flying cutting method. Cutting tools with three different materials were used in this research, namely, PCD (polycrystalline diamond) tool, CVD (chemical vapor deposition) diamond thin film coated carbide tool and uncoated carbide tool. The influence of fiber orientation on the cutting force and fracture topography were analyzed and conclusions were drawn that cutting forces are not affected by cutting speeds but significantly influenced by the fiber orientation. Cutting forces presented smaller values in the fiber orientation of 0/180° and 15/165° but the highest one in 30/150°. The fracture mechanism of carbon fibers was studied in different cutting conditions such as 0° orientation angle, 90° orientation angle, orientation angles along fiber direction, and orientation angles inverse to the fiber direction. In addition, a prediction model on the cutting defects of carbon fiber reinforced plastic was established based on acoustic emission (AE) signals.
Tech Support
Section titled “Tech Support”Original Source
Section titled “Original Source”References
Section titled “References”- 2005 - Fibre reinforced composites in aircraft construction [Crossref]
- 2008 - Composite technology and large aircraft
- 2006 - Applications and development of fiber-reinforced polymer in engineering structures
- 2002 - Machining of composite materials [Crossref]
- 1997 - Machining of fiber-reinforced composites [Crossref]
- 1985 - Machining of fibre reinforeced plastics [Crossref]
- 1995 - Orthogonal cutting mechanisms of graphite/epoxy composite. Part I: Unidirectional laminate [Crossref]
- 1995 - Orthogonal cutting mechanisms of graphite/epoxy composite. Part II: Multi-directional laminate [Crossref]
- 2003 - An experimental investigation into the orthogonal cutting of unidirectional fibre reinforced plastics [Crossref]
- 2001 - A Force Prediction Model for Cutting Unidirectional Fibre-Reinforced Plastics [Crossref]