Skip to content

Quality Factor in Polycrystalline Diamond Micromechanical Flexural Resonators

MetadataDetails
Publication Date2015-10-01
JournalJournal of Microelectromechanical Systems
AuthorsHadi Najar, Yang Chen, Amir Heidari, Liwei Lin, David A. Horsley
InstitutionsUniversity of California, Berkeley, University of California, Davis
Citations18

This paper reports an investigation into the various dissipation mechanisms that can affect polycrystalline diamond micromechanical resonators. Double-ended tuning fork and cantilever resonators were fabricated from 1-5-μm thick microcrystalline diamond films. It is shown that the quality factor of the low frequency (<;500 kHz) resonators is limited by surface loss, whereas the thermoelastic damping limits the quality factor of the higher frequency resonators. In resonators where surface loss is the dominant effect, the dependence of quality factor on resonator thickness is demonstrated. The addition of a lossy surface layer of Al <sub xmlns:mml=“http://www.w3.org/1998/Math/MathML” xmlns:xlink=“http://www.w3.org/1999/xlink”&gt;2&lt;/sub> O <sub xmlns:mml=“http://www.w3.org/1998/Math/MathML” xmlns:xlink=“http://www.w3.org/1999/xlink”&gt;3&lt;/sub> deposited via atomic layer deposition is shown to degrade quality factor, and an experiment that further demonstrates the effect of surface dissipation and results in a reduction in quality factor that scales with the thickness of the Al <sub xmlns:mml=“http://www.w3.org/1998/Math/MathML” xmlns:xlink=“http://www.w3.org/1999/xlink”&gt;2&lt;/sub> O <sub xmlns:mml=“http://www.w3.org/1998/Math/MathML” xmlns:xlink=“http://www.w3.org/1999/xlink”&gt;3&lt;/sub> layer. Heat treatment of cantilever resonators in N <sub xmlns:mml=“http://www.w3.org/1998/Math/MathML” xmlns:xlink=“http://www.w3.org/1999/xlink”&gt;2&lt;/sub> for various times up to 660 min is used to modify the resonator surface and is shown to result in a threefold increase in quality factor up to 365 000 at 26.6 kHz.

  1. 1999 - Determination of elastic modulus of thin films and small specimens using beam bending methods [Crossref]
  2. 1995 - Damping characteristics of beam-shaped micro-oscillators [Crossref]