Carbon photonics
At a Glance
Section titled āAt a Glanceā| Metadata | Details |
|---|---|
| Publication Date | 2015-11-30 |
| Journal | Quantum Electronics |
| Authors | Š. Š. ŠŠ¾Š½Š¾Š² |
| Institutions | Prokhorov General Physics Institute, National Research Nuclear University MEPhI |
| Citations | 12 |
Abstract
Section titled āAbstractāThe properties of new carbon materials (single-crystal and polycrystalline CVD diamond films and wafers, single-wall carbon nanotubes and graphene) and the prospects of their use as optical elements and devices are discussed.