Digital direct electron imaging of energy-filtered electron backscatter diffraction patterns
At a Glance
Section titled “At a Glance”| Metadata | Details |
|---|---|
| Publication Date | 2015-11-06 |
| Journal | Physical Review B |
| Authors | Stefano Vespucci, Aimo Winkelmann, G. Naresh‐Kumar, Ken Mingard, D. Maneuski |
| Institutions | University of Glasgow, Daisy Hill Hospital |
| Citations | 60 |
| Analysis | Full AI Review Included |
Direct Electron Imaging and Energy-Filtered EBSD Analysis of Diamond
Section titled “Direct Electron Imaging and Energy-Filtered EBSD Analysis of Diamond”Executive Summary
Section titled “Executive Summary”- Core Innovation: The paper demonstrates the acquisition of energy-filtered Electron Backscatter Diffraction Patterns (EBSPs) using a digital Timepix CMOS hybrid pixel detector, eliminating the traditional scintillator/CCD conversion.
- Material Focus: Validates the technique on single-crystal diamond, silicon, and GaN, comparing mass-density effects on pattern contrast.
- Low-Voltage Capability: Enables EBSP acquisition at electron beam energies ≤5 keV (down to 3 keV), significantly reducing the interaction volume.
- Spatial Resolution: Energy filtering improves spatial resolution and suppresses excess-deficiency effects, yielding higher-order Laue zone (HOLZ) ring detail.
- Acquisition Time Penalty: Achieving equivalent total electron counts at high threshold energies requires ~125× longer acquisition for diamond versus ~6× for GaN.
- Contrast Enhancement: Energy-filtered contrast improvement is most pronounced for lighter, lower-density materials—directly relevant to low-atomic-number diamond analysis.
- Practical Impact: Provides a non-destructive route to nanoscale strain mapping and lattice parameter determination with unprecedented detail.
Technical Specifications
Section titled “Technical Specifications”| Parameter | Value | Unit | Context |
|---|---|---|---|
| Beam Energy (Standard) | 20 | keV | Standard EBSP acquisition for diamond, Si, GaN |
| Beam Energy (Low-Voltage) | 3-5 | keV | Low-voltage capability of Timepix detector |
| Probe Current (Standard) | ≈10 | nA | Diamond, Si, GaN comparisons |
| Probe Current (Low-Voltage) | ≈1.5 | nA | GaN thin film at 5 keV |
| Probe Current (High-Speed) | ≈20 | nA | GaN fast acquisition tests |
| Threshold Energy (Low) | 4.6-5.5 | keV | Diamond and GaN: 5.5 keV; Si: 4.6 keV |
| Threshold Energy (High) | 19.4 | keV | Near primary beam energy for all samples |
| THL Resolution | ≈90 | eV/unit | Minimum practical discrimination step |
| Energy Resolution (Medipix2) | ≈2 | keV | Detector intrinsic energy resolution |
| Detector-to-Specimen Distance (Diamond) | ≈8 | mm | Capture angle ≈80° |
| Detector-to-Specimen Distance (Si) | ≈15 | mm | Capture angle ≈50° |
| Detector-to-Specimen Distance (GaN) | ≈10 | mm | Capture angle ≈60-70° |
| Specimen Tilt | ≈70 | ° | Sample normal relative to incident beam |
| Acquisition Time (Diamond, High Threshold) | 100 | s | 19.4 keV threshold |
| Acquisition Time (Si, High Threshold) | 1482 | s | 19.4 keV threshold |
| Acquisition Time (GaN, High Threshold) | 60 | s | 19.4 keV threshold |
| Acquisition Time (Fast Test) | 0.5-5 | ms | 20 keV, 19.4 keV threshold, GaN |
| DQE (9.1 keV threshold) | 25-26 | % | Approaching theoretical max of 27% |
| DQE (18.5 keV threshold) | 5 | % | Reduced at high threshold |
| Spatial Resolution | 8.2-11 | line pairs/mm | MTF 70%, threshold 9.1-18.5 keV |
| Pixel Array | 256×256 | pixels | Timepix hybrid pixel detector |
| Sensor Thickness | 300 | µm | Silicon sensor layer |
Key Methodologies
Section titled “Key Methodologies”- Detector Setup: Timepix CMOS hybrid pixel detector (256×256 pixels, 300 µm Si sensor) mounted in an FEI Sirion Schottky field-emission SEM in spot mode.
- Specimen Preparation: Samples tilted so normal was ~70° from the incident beam; tested materials were single-crystal diamond, silicon, and GaN thin films.
- Energy Calibration: Electron energy vs. THL (threshold) value calibrated by monitoring detector signal across a range of threshold values and incident beam energies; curves extrapolated to zero intensity.
- EBSP Acquisition (Low Threshold): Threshold set to 4.6-5.5 keV to capture all backscattered electrons contributing to pattern formation.
- EBSP Acquisition (High Threshold): Threshold set to 19.4 keV (close to 20 keV primary beam) to isolate low-loss electrons only.
- Flat-Field Correction: Raw EBSPs divided by a background image acquired by scanning the beam over a large sample area to remove detector artifacts.
- Dynamical Simulation: Bruker ESPRIT DYNAMICS software used to simulate 19.5 keV EBSPs; comparison with experimental patterns determined detector distances and capture angles.
- Comparative Analysis: Same total electron counts targeted at low and high threshold energies by adjusting acquisition times, revealing mass-density dependent contrast behavior.
6CCVD Solutions & Capabilities
Section titled “6CCVD Solutions & Capabilities”-
Applicable Materials:
- Optical Grade Single Crystal Diamond (SCD): The paper’s primary test sample was single-crystal diamond. To replicate or extend this EBSD analysis, our Optical Grade SCD (Ra < 1 nm, available in custom thicknesses from 0.1 µm to 500 µm) provides the ideal low-density, low-atomic-number substrate where energy-filtered contrast improvements are most pronounced.
- Polycrystalline Diamond (PCD): For mapping grain boundaries and texture in diamond films, our freestanding PCD plates (up to 125 mm, Ra < 5 nm) enable large-area crystallographic characterization.
-
Customization Potential:
- Dimensional Control: The paper specifies diamond samples analyzed at ~8 mm detector distances with ~80° capture angles. 6CCVD delivers custom-cut diamond in any required geometry for SEM/EBSD holder compatibility, with thicknesses from 0.1 µm freestanding films to 10 mm substrates.
- Surface Preparation: Sub-nanometer polishing (Ra < 1 nm for SCD) ensures Kikuchi pattern clarity and minimizes topographic artifacts that degrade EBSP quality.
- Metalization Options: If conductive coatings are required to mitigate charging during low-voltage (≤5 keV) SEM analysis, we provide in-house metallization with Au, Pt, Pd, Ti, W, or Cu tailored to your imaging requirements.
- Laser Cutting Services: Custom shaping to non-standard SEM mount dimensions available.
-
Engineering Support:
- 6CCVD’s in-house PhD engineering team can assist with material selection for EBSD-based crystallographic characterization, strain mapping, and lattice parameter determination projects.
- We can advise on optimal diamond grade (SCD vs. PCD), surface finish, and thickness for specific SEM voltage ranges and detector geometries relevant to your research.
-
Call to Action:
- For custom specifications or material consultation, visit 6ccvd.com or contact our engineering team directly.
View Original Abstract
Electron backscatter diffraction is a scanning electron microscopy technique used to obtain crystallographic information on materials. It allows the nondestructive mapping of crystal structure, texture, and strain with a lateral and depth resolution on the order of tens of nanometers. Electron backscatter diffraction patterns (EBSPs) are presently acquired using a detector comprising a scintillator coupled to a digital camera, and the crystallographic information obtainable is limited by the conversion of electrons to photons and then back to electrons again. In this article we will report the direct acquisition of energy-filtered EBSPs using a digital complementary metal-oxide-semiconductor hybrid pixel detector, Timepix. We show results from a range of samples with different mass and density, namely diamond, silicon, and GaN. Direct electron detection allows the acquisition of EBSPs at lower $(\ensuremath{\le}5$ keV) electron beam energies. This results in a reduction in the depth and lateral extension of the volume of the specimen contributing to the pattern and will lead to a significant improvement in lateral and depth resolution. Direct electron detection together with energy filtering (electrons having energy below a specific value are excluded) also leads to an improvement in spatial resolution but in addition provides an unprecedented increase in the detail in the acquired EBSPs. An increase in contrast and higher-order diffraction features are observed. In addition, excess-deficiency effects appear to be suppressed on energy filtering. This allows the fundamental physics of pattern formation to be interrogated and will enable a step change in the use of electron backscatter diffraction (EBSD) for crystal phase identification and the mapping of strain. The enhancement in the contrast in high-pass energy-filtered EBSD patterns is found to be stronger for lighter, less dense materials. The improved contrast for such materials will enable the application of the EBSD technique to be expanded to materials for which conventional EBSD analysis is not presently practicable.
Tech Support
Section titled “Tech Support”Original Source
Section titled “Original Source”References
Section titled “References”- 2009 - Electron Backscatter Diffraction in Materials Science
- 2003 - Scanning Electron Microscopy and X-ray Microanalysis [Crossref]
- 2009 - Electron Backscatter Diffraction in Materials Science
- 2009 - Electron Backscatter Diffraction in Materials Science
- 2009 - Electron Backscatter Diffraction in Materials Science