Skip to content

Optically pumped DBR-free semiconductor disk lasers

MetadataDetails
Publication Date2015-12-16
JournalOptics Express
AuthorsZhou Yang, Alexander R. Albrecht, Jeffrey G. Cederberg, Mansoor Sheik‐Bahae
InstitutionsSandia National Laboratories, University of New Mexico
Citations70
AnalysisFull AI Review Included
  • Breakthrough Architecture: Successful demonstration of high-power, room-temperature, broadly tunable DBR-free (Distributed Bragg Reflector-free) Semiconductor Disk Lasers (SDLs).
  • Thermal Management Innovation: Elimination of the thick, high thermal impedance semiconductor DBR by lifting off the multi-quantum-well (MQW) active region and bonding it directly to a transparent single-crystalline CVD diamond heatspreader.
  • Record Performance: Achieved a maximum continuous-wave (CW) output power of 2.5 W and a record wavelength tuning range of 78 nm centered at ~1160 nm.
  • Material Versatility: Validated operation in both standard transmission geometry and a novel Total Internal Reflection (TIR) geometry, significantly relaxing lattice-matching requirements typical of conventional VECSELs.
  • Power Scaling Potential: Thermal modeling demonstrates that a “dual heatspreader” (sandwiched) DBR-free architecture offers superior heat extraction compared to standard VECSELs, paving the way for >100 W class devices.
  • Process Compatibility: Used standard epitaxial lift-off and Van der Waals bonding techniques (originally developed for GaAs) applied to strained InGaAs MQWs, establishing a scalable pathway for heterogeneous integration.
ParameterValueUnitContext
Maximum CW Output Power2.5WDBR-free SDL with single-crystal diamond heatspreader
Wavelength Tuning Range78nmRecord for DBR-free SDLs
Center Wavelength≈ 1160nmStrained InGaAs/GaAs MQW emission
Pump Wavelength808nmIndium-bonded pump diode
Wall-Plug Efficiency (Max Power)~12.5%At 2.5 W output, ~20 W pump
Heatspreader MaterialSingle-Crystal CVD Diamond-Superior thermal conductivity vs. standard DBR
Active Region StructureStrained InGaAs MQW-10 pairs of quantum wells
Cavity Geometries DemonstratedTransmission & Total Internal Reflection (TIR)-Validates DBR-free concept
DBR Pairs Eliminated20-30 (typical)pairsRemoves ~3-5 µm of resistive epitaxial material
Predicted ΔT (Dual Heatspreader Model)< 30KAt 250 W pump power (thermal model)
Reference Sample Tuning (1046 nm device)900 - 1100nmDemonstrates broadband gain bandwidth
  • Epitaxial Growth: Growth of strained InGaAs/GaAs multi-quantum-well (MQW) active regions on GaAs substrates, separated by a thin AlAs sacrificial layer.
  • Epitaxial Lift-Off (ELO): Selective wet chemical etching of the AlAs sacrificial layer to release the thin MQW active membrane from the growth substrate.
  • Van der Waals Bonding: Transfer and bonding of the MQW membrane onto transparent heatspreader substrates (single-crystal CVD diamond, sapphire, ZnSe, BaF2) via surface tension forces.
  • Cavity Construction: Implementation of an external cavity design utilizing an output coupler (OC) and a high-reflectivity (HR) curved dielectric mirror; no semiconductor DBR used.
  • Optical Pumping: 808 nm fiber-coupled diode laser delivering up to ~20 W incident power, focused to a ~390 µm spot size.
  • Thermal Modeling: Finite-element heat transfer analysis comparing (a) traditional VECSEL, (b) DBR-free SDL, (c) thin-device with single heatspreader, and (d) DBR-free SDL with dual heatspreaders.
  • Applicable Materials: This research relies on the use of Optical-Grade Single Crystal Diamond (SCD) to function as an intra-cavity heatspreader for the InGaAs MQW membrane. To replicate or extend this work, 6CCVD supplies high-purity SCD substrates with industry-leading thermal conductivity (>1800 W/m·K). 6CCVD also provides freestanding SCD membranes in the 0.1 µm - 500 µm thickness range, ideal for bonding to GaAs-based III-V epitaxial structures.
  • Customization Potential: The lift-off and Van der Waals bonding process used in the paper demands exceptionally flat, ultra-smooth surfaces. 6CCVD delivers SCD polished to Ra < 1 nm, ensuring void-free Van der Waals bonding. Furthermore, if a dual-heatspreader (sandwich) architecture is required for power scaling >100 W, 6CCVD can provide custom thicknesses and laser-cut dimensions to match the specific active region footprint.
  • Engineering Support: Transitioning from a single-crystal diamond heatspreader to a fully integrated dual-diamond “sandwich” device requires precise control of bonding interfaces, surface preparation, and managing strain in highly strained InGaAs MQWs. 6CCVD’s in-house PhD engineering team can assist with material selection, surface preparation specifications, and bonding compatibility for next-generation VECSEL and SDL thermal management projects.
  • Call to Action: For custom specifications, ultra-thin diamond membranes, or material consultation for advanced laser cooling and high-power laser projects, visit 6ccvd.com or contact our engineering team directly.
View Original Abstract

We report high power distributed Bragg reflector (DBR)-free semiconductor disk lasers. With active regions lifted off and bonded to various transparent heatspreaders, the high thermal impedance and narrow bandwidth of DBRs are mitigated. For a strained InGaAs multi-quantum-well sample bonded to a single-crystalline chemical-vapor deposited diamond, a maximum CW output power of 2.5 W and a record 78 nm tuning range centered at λ≈1160 nm was achieved. Laser operation using a total internal reflection geometry is also demonstrated. Furthermore, analysis for power scaling, based on thermal management, is presented.