Diamond crystallization and growth in N–H enriched environment under HPHT conditions
At a Glance
Section titled “At a Glance”| Metadata | Details |
|---|---|
| Publication Date | 2016-01-01 |
| Journal | CrystEngComm |
| Authors | Xiaobing Liu, Xiaopeng Jia, Chao Fang, Hongan Ma |
| Institutions | Jilin University, Northwestern University |
| Citations | 25 |
Abstract
Section titled “Abstract”Advances in understanding the state and transformation of impurity-related defects in natural diamond have been achieved by means of high-pressure and high-temperature annealing experiments. However, the existing literature featuring complex behaviors of aggregated nitrogen and hydrogen-related defect (3107 cm−1 center) has remained controversial. Their formation mechanism during diamond crystallization is still unclear, thus further investigation is required. In this work, we have successfully synthesized a variety of high-quality diamonds containing nitrogen impurities with IaA (nitrogen pairs), IaB (group of four nitrogen atoms around a vacancy) and Ib (single-substitutional nitrogen) characteristics ranging from <1 ppm to 3380 ppm at pressures ranging from 5.0 GPa to 6.3 GPa and temperatures of 1300-1650 °C. Our results provide new experimental evidence for the aggregation of nitrogen impurities (A- and B-centers) during diamond growth. We notice that the hydrogen is easily trapped by nitrogen atoms to form nitrogen-hydrogen complexes (-NH, -NH2, -NH3) when the nitrogen tends to form C-centers in hydrogen-enriched environments. Additionally, we observed that the high reaction temperature and formation of A-centers during diamond growth play important roles in the formation of the 3107 cm−1 center. We believe the current results could be helpful for further understanding and constructing a clear model of impurity-related defects, and thus provide us deeper insights into the genesis of natural diamond.
Tech Support
Section titled “Tech Support”Original Source
Section titled “Original Source”References
Section titled “References”- 2013 - HPHT-treated diamonds [Crossref]