Diamond detectors with electrodes graphitized by means of laser
At a Glance
Section titled āAt a Glanceā| Metadata | Details |
|---|---|
| Publication Date | 2016-01-01 |
| Journal | Virtual Community of Pathological Anatomy (University of Castilla La Mancha) |
| Authors | Mary De Feudis, Anna Paola Caricato, G. Chiodini, Mark Martino, Giuseppe Maruccio |
| Citations | 3 |
Abstract
Section titled āAbstractāIn the last years there has been an increase of interest in diamond devices because of the promising applications in different field, such as high-energy physics, radiotherapy and biochemical applications. In particular, a new frontier is represented by the realization of full-carbon detectors characterized by graphite electrodes, which give to the devices considerable advantages like high radiation hardness, perfect mechanical adhesion and good charge collection properties. In this paper the manufacturing of full-carbon devices and their detection performances are illustrated and compared to a reference diamond detector characterized by traditional electrodes.