Electrochemical behavior of new electrode material - Compact of boron-doped synthetic diamond

MetadataDetails
Publication Date2016-01-01
JournalRussian Journal of Electrochemistry
AuthorsYu. V. Pleskov, M. D. Кrotova, Š’. Š’. Елкин, Š•. А. Екимов
InstitutionsFrumkin Institute of Physical Chemistry and Electrochemistry, Institute for High Pressure Physics
Citations13

Electrochemical properties of new electrode material—compact of boron-doped synthetic diamond—is studied for the first time. Cylindrical samples 3.5-4 mm in diameter and 2.5 mm in height were obtained by thermobaric processing of graphite-boron carbide mixtures in the diamond thermodynamic stability region (at the pressure of 8-9 GPa and temperature of ~2500 K). Their electrode behavior is studied using cyclic voltammetry and electrochemical impedance spectroscopy techniques. The cyclic voltammograms of the compact samples showed that their electrode characteristics are similar to those of traditional thin-film diamond electrodes obtained by the chemical vapor deposition (CVD) technique. In particular, they demonstrate rather wide potential window, low background current in indifferent electrolytes, and good reproducibility. It can be concluded that the diamond compacts practically are not inferior to the thin-film CVD-diamond electrodes and can serve as indicator electrodes, e.g., in electroanalysis. At the same time their compact form may be a convenience in the designing of electrolyzers and other electrochemical devices.

  1. 2003 - Elektrokhimiya almaza
  2. 2005 - Electrochemistry of Diamond
  3. 2011 - Synthetic Diamond Films: Preparation, Electrochemistry, Characterization and Applications [Crossref]