Femtosecond Laser Machining of Micron-Diameter Graphitized Columns in Diamond
At a Glance
Section titled āAt a Glanceā| Metadata | Details |
|---|---|
| Publication Date | 2016-01-01 |
| Journal | Conference on Lasers and Electro-Optics |
| Authors | Brian K. Canfield, Tom Wulz, Eric Lukosi, Stefan Spanier, Lloyd M. Davis |
| Institutions | University of Tennessee at Knoxville, Knoxville College |
Abstract
Section titled āAbstractāGraphitized columns with ~1 μm diameter through ~500 μm-thick diamonds are formed by femtosecond laser machining using both aberration-corrected and Bessel beam focusing with high numerical aperture for development of radiation-hard, high-energy particle detectors.