Single Defect Centers in Wide-bandgap Materials - Stable, Bright and Pure Quantum Light Sources
At a Glance
Section titled âAt a Glanceâ| Metadata | Details |
|---|---|
| Publication Date | 2016-01-01 |
| Authors | Tim Schröder |
Abstract
Section titled âAbstractâA promising class of single photon emitters consists of crystal defect centers in wide-bandgap materials. Here, we introduce, discuss, and compare such color centers in established and new materials including diamond, silicon carbide, and boron and gallium nitride.