Surface characteristics and damage distributions of diamond wire sawn wafers for silicon solar cells

MetadataDetails
Publication Date2016-01-01
JournalAIMS Materials Science
AuthorsBhushan Sopori, Srinivas Devayajanam, Prakash Basnyat
InstitutionsNational Renewable Energy Laboratory, New Jersey Institute of Technology
Citations19

This paper describes surface characteristics, in terms of its morphology, roughness and near-surface damage of Si wafers cut by diamond wire sawing (DWS) of Si ingots under different cutting conditions. Diamond wire sawn Si wafers exhibit nearly-periodic surface features of different spatial wavelengths, which correspond to kinematics of various movements during wafering, such as ingot feed, wire reciprocation, and wire snap. The surface damage occurs in the form of frozen-in dislocations, phase changes, and microcracks. The in-depth damage was determined by conventional methods such as TEM, SEM and angle-polishing/defect-etching. However, because these methods only provide local information, we have also applied a new technique that determines average damage depth over a large area. This technique uses sequential measurement of the minority carrier lifetime after etching thin layers from the surfaces. The lateral spatial damage variations, which seem to be mainly related to wire reciprocation process, were observed by photoluminescence and minority carrier lifetime mapping. Our results show a strong correlation of damage depth on the diamond grit size and wire usage.

  1. 2003 - Fixed abrasive diamond wire machining—part I: process monitoring and wire tension force [Crossref]
  2. 2012 - Thin Czochralski silicon solar cells based on diamond wire sawing technology [Crossref]
  3. 2006 - Wafering of silicon crystals [Crossref]
  4. 2015 - Surface damage and mechanical strength of silicon wafers [Crossref]
  5. 2012 - A state-of-the-art review of ductile cutting of silicon wafers for semiconductor and microelectronics industries [Crossref]
  6. 1990 - Ductile- regime machining of germanium and silicon [Crossref]
  7. 2015 - Wire-sawing processes: parametrical study and modeling [Crossref]
  8. 2002 - Phase transformation in silicon under contact loading [Crossref]
  9. 2016 - A method for determining average damage depth of sawn crystalline silicon wafers [Crossref]
  10. 2015 - Surface damage introduced by diamond wire sawing of Si wafers: Measuring in-depth and the lateral distributions for different cutting parameters [Crossref]