Removal of herbicide glyphosate by conductive-diamond electrochemical oxidation
At a Glance
Section titled âAt a Glanceâ| Metadata | Details |
|---|---|
| Publication Date | 2016-02-03 |
| Journal | Applied Catalysis B: Environmental |
| Authors | Humberto RubĂ-JuĂĄrez, Salvador Cotillas, Cristina SĂĄez, Pablo Cañizares, Carlos Barrera-DĂaz |
| Institutions | University of Castilla-La Mancha, Universidad Autónoma del Estado de México |
| Citations | 101 |
Abstract
Section titled âAbstractâThis work focuses on the removal of herbicide glyphosate by electrolysis with boron doped diamond anodes. Both the electrolysis of the pure reagent and that of a commercial dispersion (RoundUp) are evaluated. Results show that it is possible to attain a complete mineralization of this herbicide and point out the key role of the supporting electrolyte in the efficiency of the process. This role is explained in terms of the electrogeneration of oxidants. The electrolysis of glyphosate also leads to the release of phosphate and nitrate anions. Further electrochemical and chemical reactivity explains the occurrence of ammonium and other nitrogen species in the electrolyte during the process. Regarding the influence of the type of herbicide (chemical or commercial), competitive reactions have been observed between the electrolysis of herbicide and surfactant, which help to explain the lower efficiency observed in the degradation of RoundUp. Regarding the influence of the operation current density, the process is found to be more efficient at low current densities but at these conditions it is not possible to attain the complete mineralization of pollutant.