(Invited) Diamond - the Unknowns and Challenges to Make It Work for GaN Electronics

MetadataDetails
Publication Date2016-04-01
JournalECS Meeting Abstracts
AuthorsMartin Kuball, J. Anaya, Dong Liu, Roland Baranyai, Huarui Sun
InstitutionsUniversity of Bristol

Diamond has demonstrated excellent properties for thermal management of GaN electronics. In this presentation, we review our latest results on the diamond properties near the GaN-on-diamond interface, and the mechanical stability of the GaN-on-diamond interface and its properties.