Skip to content

Time Dependent DD Neutrons Measurement Using a Single Crystal Chemical Vapor Deposition Diamond Detector on EAST

MetadataDetails
Publication Date2016-08-30
JournalPlasma Science and Technology
AuthorsTengfei Du, Xingyu Peng, Zhongjing Chen, Zhimeng Hu, Lijian Ge
InstitutionsPeking University, State Key Laboratory of Nuclear Physics and Technology
Citations12

A single crystal chemical vapor deposition (scCVD) diamond detector has been successfully employed for neutron measurements in the EAST (Experimental Advanced Superconducting Tokamak) plasmas. The scCVD diamond detector coated with a 5 μm 6LiF (95% 6Li enriched) layer was placed inside a polyethylene moderator to enhance the detection efficiency. The time-dependent neutron emission from deuteron plasmas during neutral beam injection (NBI) heating was obtained. The measured results are compared with that of fission chamber detectors, which always act as standard neutron flux monitors. The scCVD diamond detector exhibits good reliability, stability and the capability to withstand harsh radiation environments despite its low detection efficiency due to the small active volume.