Bulk and surface properties of ZnTe–ZnS system semiconductors
At a Glance
Section titled “At a Glance”| Metadata | Details |
|---|---|
| Publication Date | 2016-09-16 |
| Journal | Russian Journal of Physical Chemistry A |
| Authors | I. A. Kirovskaya, Е. В. Миронова, Б. А. Косарев, П. Е. Нор, Т. Л. Букашкина |
| Institutions | Omsk State Technical University |
| Citations | 5 |
Abstract
Section titled “Abstract”Physicochemical studies of a new ZnTe-ZnS semiconductor system are conducted. It is found that at certain ratios of binary components, substitutional solid solutions with a cubic sphalerite structure are formed in this system. Interrelated laws governing changes in the bulk (crystal chemical, structural) and surface (acid-base) properties with varying system composition are identified. It is assumed they can be attributed to the nature of the active (acid-base) sites. The presented data, observed patterns, and an interpretation of them are used not only to confirm earlier proposed mechanisms of atomic-molecular interaction on diamond-like semiconductors, but to search for promising materials for use in highly sensitive selective sensors for environmental and medical purposes as well.
Tech Support
Section titled “Tech Support”Original Source
Section titled “Original Source”References
Section titled “References”- 2010 - Solid Solutions of Binary and Multicomponent Semiconductor Systems
- 2012 - Surface Properties of Binary Diamond-Like Semiconductors
- 1970 - X-ray and Electron Optical Analysis
- 1961 - Handbook on X-ray Structural Analysis
- 2007 - Microscopy Techniques for Material Study
- 1988 - Surface Properties of Diamond-like Semiconductors. Chemical Composition of the Surface. Catalysis
- 2001 - Surface Phenomena
- 1967 - Acid-Base Titration in Nonaqueous Solutions
- 1988 - Surface Properties of Binary Diamondlike Semiconductors. Chemical Composition of the Surface. Catalysis