Interatomic bond energy and analytical scale of hardness
At a Glance
Section titled “At a Glance”| Metadata | Details |
|---|---|
| Publication Date | 2017-01-01 |
| Journal | Journal of Superhard Materials |
| Authors | А. В. Лысенко |
| Institutions | V. Bakul Institute for Superhard Materials, National Academy of Sciences of Ukraine |
| Citations | 3 |
Abstract
Section titled “Abstract”Based on detailed models of interatomic cohesion and the well-developed structural-thermodynamic approach, the interatomic bond energy has been determined for some covalent and metallic crystals and it has been found to agree with experimental data. Using the proposed analytical relationship for the degree of covalency of crystals the author has elaborated a generalized model that describes experimental hardness of supersclerometer materials (diamond, cBN, SiC, and others), minerals, refractory compounds, semiconductors, ionic crystals and metals. On the basis of the mechanical-chemical approach to (nano)flow a dislocation model of crystal-mechanical anisotropy of yield strength has been put forward for monocrystalline diamond and lonsdaleite; the model makes it possible to draw a conclusion on a slight difference in their sclerometric characteristics. The experimental relationships that govern high-temperature high-pressure plasticity in some covalent crystals are discussed.
Tech Support
Section titled “Tech Support”Original Source
Section titled “Original Source”References
Section titled “References”- 1987 - Fizicheskie svoistva almaza: Spravochnik
- 1993 - Sintez, spekanie i svoistva kubicheskogo nitrida bora
- 2002 - Sintez sverkhtverdykh materialov
- 1978 - Stroenie veshchestva
- 1965 - Fiziko-khimicheskie svoistva elementov. Spravochnik
- 1961 - Valence
- 1976 - Tablitsy fizicheskikh velichin. Spravochnik
- 1980 - Sverkhtverdye materialy