A new family of multifunctional silicon clathrates - Optoelectronic and thermoelectric applications

MetadataDetails
Publication Date2017-02-28
JournalJournal of Applied Physics
AuthorsYinqiao Liu, Xue Jiang, Yingying Huang, Si Zhou, Jijun Zhao
InstitutionsDalian University of Technology
Citations16

To develop Si structures for multifunctional applications, here we proposed four new low-density silicon clathrates (Si-CL-A, Si-CL-B, Si-CL-C, and Si-CL-D) based on the same bonding topologies of clathrate hydrates. The electronic and thermal properties have been revealed by first-principles calculations. By computing their equation of states, phonon dispersion, and elastic constants, the thermodynamic, dynamic, and mechanical stabilities of Si-CL-A, Si-CL-B, Si-CL-C, and Si-CL-D allotropes are confirmed. In the low-density region of the phase diagram, Si-CL-B, Si-CL-D, and Si-CL-C would overtake diamond silicon and type II clathrate (Si-CL-II) and emerge as the most stable Si allotropes successively. Among them, the two direct semiconductors with bandgaps of 1.147 eV (Si-CL-A) and 1.086 eV (Si-CL-D) are found. The suitable bandgaps close to the optimal Shockley-Queisser limit result in better absorption efficiency in solar spectrum than conventional diamond silicon. Owing to the unique cage-based framework, the thermal conductivity of these Si allotropes at room temperature are very low (2.7-5.7 Wmāˆ’1 Kāˆ’1), which are lower than that of diamond structured Si by two orders of magnitude. The suitable bandgaps, small effective masses, and low thermal conductivity of our new silicon allotropes are anticipated to find applications in photovoltaic and thermoelectric devices.

  1. 2001 - Semiconductors and Semimetals