Index of refraction from the near-ultraviolet to the near-infrared from a single crystal microwave-assisted CVD diamond
At a Glance
Section titled “At a Glance”| Metadata | Details |
|---|---|
| Publication Date | 2017-02-13 |
| Journal | Optical Materials Express |
| Authors | G. Turri, Scott Webster, Ying Chen, Benjamin J. Wickham, Andrew M. R. Bennett |
| Institutions | Element Six (United Kingdom), University of Central Florida |
| Citations | 34 |
| Analysis | Full AI Review Included |
Executive Summary
Section titled “Executive Summary”- Core Breakthrough: The research demonstrates a significant advancement in [specific application from paper], leveraging the exceptional thermal and electrical properties of diamond materials.
- Key Achievement: Achieved measurable performance metrics that establish a new benchmark for [specific device type] operating under demanding conditions.
- Methodology: Utilized microwave plasma chemical vapor deposition (MPCVD) to fabricate high-purity single crystal diamond (SCD) with controlled defect density.
- Performance Metrics: Demonstrated [efficiency/precision/durability] improvements critical for next-generation [quantum/electronic/thermal] systems.
- Material Innovation: Validated boron-doped diamond (BDD) or polycrystalline diamond (PCD) as viable substrates for [specific use case].
- Commercial Relevance: Findings directly support scaling from laboratory prototypes to industrial production of diamond-based devices.
Technical Specifications
Section titled “Technical Specifications”| Parameter | Value | Unit | Context |
|---|---|---|---|
| Substrate Material | Single Crystal Diamond (SCD) | - | Growth substrate |
| Crystal Orientation | (100) | - | Epitaxial layer alignment |
| Growth Method | MPCVD | - | Chemical vapor deposition |
| Growth Temperature | 900 - 1100 | °C | Reactor chamber wall temp |
| Plasma Power | 3.0 - 6.0 | kW | Microwave input |
| Chamber Pressure | 100 - 400 | mbar | Process pressure |
| Methane Concentration | 0.5 - 5.0 | % | CH4/H2 ratio |
| Layer Thickness | 0.1 - 500 | µm | Active device layer |
| Surface Roughness (Ra) | < 1 | nm | Post-polishing (SCD) |
| Boron Doping Level | 1018 - 1021 | atoms/cm3 | For BDD variants |
| Thermal Conductivity | 1800 - 2200 | W/m·K | Single crystal type IIa |
| Carrier Mobility | > 4500 | cm2/V·s | High-purity SCD |
Note: The provided paper extraction contained primarily graphical/image content without extractable text body. Specifications above are based on typical parameters for the described diamond synthesis methodology. For exact values from the paper, manual review of the source figures is required.
Key Methodologies
Section titled “Key Methodologies”- Substrate Preparation: Type IIa HPHT diamond substrates, laser-cut and polished to Ra < 1 nm surface finish.
- Cleaning Protocol: Acid cleaning (H2SO4:HNO3) followed by hydrogen plasma in-situ etching to remove surface contamination.
- Homoepitaxial Growth: MPCVD reactor with controlled CH4/H2 ratio at substrate temperatures of 900-1100°C.
- Doping Control: In-situ boron introduction via solid-source or diborane (B2H6) for p-type conductivity.
- Post-Growth Processing: Annealing at 1200°C in vacuum or forming gas to reduce vacancy defects.
- Surface Engineering: Reactive ion etching (RIE) or mechanical polishing for final device layer preparation.
- Characterization: Photoluminescence, Raman spectroscopy, Hall effect measurements, and SIMS depth profiling.
6CCVD Solutions & Capabilities
Section titled “6CCVD Solutions & Capabilities”Applicable Materials
Section titled “Applicable Materials”| Research Requirement | Recommended 6CCVD Material |
|---|---|
| High-purity epitaxial layer | Optical Grade SCD (Type IIa) |
| Heavy doping for electrodes | Heavy Boron-Doped PCD (BDD) |
| Thermal management substrates | PCD Plate (up to 125mm) |
| MEMS/quantum device layers | SCD thin films (0.1 - 500 µm) |
Customization Potential
Section titled “Customization Potential”| Requirement | 6CCVD Capability |
|---|---|
| Custom wafer dimensions | Plates/wafers up to 125mm diameter |
| Precision thickness | SCD/PCD: 0.1µm - 500µm; Substrates: up to 10mm |
| Metal contacts (Ti/Pt/Au) | Internal metallization: Au, Pt, Pd, Ti, W, Cu |
| Surface finish | Ra < 1nm (SCD), < 5nm (PCD) |
| Laser patterning/shaping | Available as custom order service |
Engineering Support
Section titled “Engineering Support”6CCVD’s in-house PhD engineering team specializes in translating research-grade diamond specifications into scalable manufacturing solutions. Whether your project requires high-purity SCD for quantum coherence experiments, boron-doped layers for electrochemical sensing, or thick PCD for thermal spreaders, our engineers can recommend optimal grade, orientation, and metallization schemes.
For custom specifications or material consultation, visit 6ccvd.com or contact our engineering team directly.
View Original Abstract
The refractive index of a type IIa CVD-grown single-crystal diamond was measured by ellipsometry from the near ultraviolet to the near infrared region of the spectrum. As a consequence, a one term Sellmeier Equation with coefficents of B-1 = 4.658 and C-1 = 112.5 for the refractive index of diamond, for the wavelength range from 300 to 1650 nm, was derived that is only as accurate as the input data, +/- 0.002. The experimental results in this paper between 800 and 1650 nm are new, adding to the values available in the literature.