Diamond anvil cell using metallic diamond electrodes
At a Glance
Section titled āAt a Glanceā| Metadata | Details |
|---|---|
| Publication Date | 2017-03-09 |
| Journal | Japanese Journal of Applied Physics |
| Authors | Ryo Matsumoto, Tetsuo Irifune, Masashi Tanaka, Hiroyuki Takeya, Yoshihiko Takano |
| Institutions | Ehime University, National Institute for Materials Science |
| Citations | 22 |
Abstract
Section titled āAbstractāA novel diamond anvil cell specialized for resistivity measurements under high pressure have been developed. Boron-doped metallic diamond electrodes were deposited onto a nano-polycrystalline diamond anvil using a microwave plasma-assisted chemical vapor deposition technique combined with electron beam lithography. The various designs of boron-doped metallic diamond electrodes were demonstrated, and they showed no signs of degradation after repeated compression.