Nanoscale Engineering of Closely-Spaced Electronic Spins in Diamond

MetadataDetails
Publication Date2017-03-17
JournalBulletin of the American Physical Society
AuthorsDiego Scarabelli, Matt Trusheim, Ophir Gaathon, Dirk Englund, Shalom J. Wind

Numerous theoretical protocols have been developed for quantum information processing with dipole-coupled solid-state spins. Nitrogen vacancy (NV) centers in diamond have many of the desired properties, but a central challenge has been the positioning of NV centers at the nanometer scale that would allow for efficient and consistent dipolar couplings. Here we demonstrate a method for chip-scale fabrication of arrays of single NV centers with record spatial localization of about 10 nm in all three dimensions and controllable inter-NV spacing as small as 40 nm, which approaches the length scale of strong dipolar coupling. Our approach uses masked implantation of nitrogen through nanoapertures in a thin gold film, patterned via electron-beam lithography and dry etching. We verified the position and spin properties of the resulting NVs through wide-field super-resolution optically detected magnetic resonance imaging.