Preparation of boron doped diamond modified by iridium for electroreduction of carbon dioxide (CO2)
At a Glance
Section titled āAt a Glanceā| Metadata | Details |
|---|---|
| Publication Date | 2017-04-01 |
| Journal | IOP Conference Series Materials Science and Engineering |
| Authors | Andi Muhammad Ichzan, Jarnuzi Gunlazuardi, Tribidasari A. Ivandini |
| Institutions | University of Indonesia |
| Citations | 5 |
Abstract
Section titled āAbstractāElectroreduction of carbon dioxide (CO2) at iridium oxide-modified boron-doped diamond (IrOx-BDD) electrodes in aqueous electrolytes was studied by voltammetric method. The aim of this study was to find out the catalytic effect of IrOx to produce fine chemicals contained of two or more carbon atoms (for example acetic acid) in high percentage. Characterization using FE-SEM and XPS indicated that IrO2 can be deposited at BDD electrode, whereas characterization using cyclic voltammetry indicated that the electrode was applicable to be used as working electrode for CO2 electroreduction.