Cascaded continuous-wave Raman frequency conversion in external-cavity diamond lasers
At a Glance
Section titled āAt a Glanceā| Metadata | Details |
|---|---|
| Publication Date | 2017-06-01 |
| Authors | Robert J. Williams, David J. Spence, Oliver Lux, Richard P. Mildren |
| Institutions | Deutsches Zentrum für Luft- und Raumfahrt e. V. (DLR), Macquarie University |
| Citations | 2 |
Abstract
Section titled āAbstractāWe report efficient, high-power cw frequency conversion in diamond from 1-1.5 µm via the second Stokes shift, and an analytical model highlighting the possibility of extension to higher cascaded Stokes shifts.