A novel approach of deposition for uniform diamond films on circular saw blades

MetadataDetails
Publication Date2017-09-15
JournalPlasma Science and Technology
AuthorsHongxiu Zhou, Boya Yuan, Jilei Lyu, Nan Jiang
InstitutionsDalian University of Technology, Ningbo Institute of Industrial Technology
Citations7

Uniform diamond films are highly desirable for cutting industries, due to their high performance and long lifetime used on cutting tools. Nevertheless, they are difficult to obtain on cutting tools with complicated shapes, greatly limiting the applications of diamond films. In this study, a novel approach of deposition for uniform diamond films is proposed, on circular saw blades made of cemented carbide using reflectors of brass sheets. Diamond films are deposited using hot filament chemical vapor deposition (HFCVD). A novel concave structure of brass sheets is designed and fabricated, improving the distribution of temperature field, and overcoming the disadvantages of the conventional HFCVD systems. This increases the energy efficiency of use without changing the structure and increasing the cost of HFCVD. The grains are refined and the intensities of diamond peaks are strengthened obviously, which is confirmed by scanning electron microscopy and Raman spectra respectively.