A Proposal of NV Center in Nanodiamond Based Magnetometer toward Human Neuron AP Detection
At a Glance
Section titled āAt a Glanceā| Metadata | Details |
|---|---|
| Publication Date | 2017-09-01 |
| Authors | Heng Yuan, Jixing Zhang, Chen Zhang, Ning Zhang, Lixia Xu |
| Institutions | Beihang University |
Abstract
Section titled āAbstractāHuman neuron action potential detection has a great application in the field of neurosciences and neurotherapy. However, traditional technology can hardly perform a non-invasive action potential (AP) detection for small axon such as human neuron axon. We propose a new AP detection method by measuring the AP induced magnetic pulse signal utilizing nitrogen vacancy (NV) centers in nanodiamond. This method can theoretically achieve effective detection of a 10 μm diameter neuron axon.
Tech Support
Section titled āTech SupportāOriginal Source
Section titled āOriginal SourceāReferences
Section titled āReferencesā- 2006 - Characterization and application of single fluorescent nanodiamonds as cellular biomarkers [Crossref]
- 2014 - In vivo imaging and tracking of individual nanodiamonds in drosophila melanogaster embryos [Crossref]