Symmetry and Structure of Cubic Semiconductor Surfaces
At a Glance
Section titled āAt a Glanceā| Metadata | Details |
|---|---|
| Publication Date | 2017-10-17 |
| Journal | Langmuir |
| Authors | Stephen J. Jenkins |
| Institutions | University of Cambridge |
| Citations | 1 |
Abstract
Section titled āAbstractāA systematic stereographic approach to the description of surface symmetry and structure, applied previously to face-centered cubic, body-centered cubic, and hexagonal close-packed metals, is here extended to the surfaces of diamond-structure and zinc-blende-structure semiconductors. A variety of symmetry-structure combinations are categorized and the chiral properties of certain cases emphasized. A general condition for nonpolarity in the surfaces of zincblende materials is also noted.