Luminescence Spectroscopy of Bound Excitons in Diamond (Phys. Status Solidi A 11∕2017)
At a Glance
Section titled “At a Glance”| Metadata | Details |
|---|---|
| Publication Date | 2017-11-01 |
| Journal | physica status solidi (a) |
| Authors | Julien Barjon |
| Institutions | Centre National de la Recherche Scientifique, Groupe d’Étude de la Matière Condensée |
| Citations | 1 |
Abstract
Section titled “Abstract”Since the research on diamond doping remains an issue for electronic applications, the luminescence spectroscopy of bound excitons appears essential to evaluate the properties of shallow dopants in diamond. In this paper (article No. 201700402), the formation and recombination processes of bound excitons in diamond are reviewed for boron acceptors, phosphorus, and arsenic donors. Pulsed and continuous excitations are considered, the latter being currently used for the measurement of donor and acceptor concentrations in diamond.