Skip to content

Surface Texturing of CVD Diamond Assisted by Ultrashort Laser Pulses

MetadataDetails
Publication Date2017-11-03
JournalCoatings
AuthorsD.M. Trucchi, A. Bellucci, M. Girolami, Matteo Mastellone, S. Orlando
InstitutionsInstitute of Structure of Matter
Citations61

Diamond is a wide bandgap semiconductor with excellent physical properties which allow it to operate under extreme conditions. However, the technological use of diamond was mostly conceived for the fabrication of ultraviolet, ionizing radiation and nuclear detectors, of electron emitters, and of power electronic devices. The use of nanosecond pulse excimer lasers enabled the microstructuring of diamond surfaces, and refined techniques such as controlled ablation through graphitization and etching by two-photon surface excitation are being exploited for the nanostructuring of diamond. On the other hand, ultrashort pulse lasers paved the way for a more accurate diamond microstructuring, due to reduced thermal effects, as well as an effective surface nanostructuring, based on the formation of periodic structures at the nanoscale. It resulted in drastic modifications of the optical and electronic properties of diamond, of which ā€œblack diamondā€ films are an example for future high-temperature solar cells as well as for advanced optoelectronic platforms. Although experiments on diamond nanostructuring started almost 20 years ago, real applications are only today under implementation.

  1. 2016 - Diamond device architectures for UV laser monitoring [Crossref]
  2. 2012 - Diamond detectors for UV and X-ray source imaging [Crossref]
  3. 2012 - Very fast and priming-less single-crystal diamond X-ray dosimeters [Crossref]
  4. 2015 - Mosaic diamond detectors for fast neutrons and large ionizing radiation fields [Crossref]
  5. 2016 - Thick homoepitaxial (110)-oriented phosphorus-doped n-type diamond [Crossref]
  6. 2016 - Heavily phosphorus-doped nano-crystalline diamond electrode for thermionic emission application [Crossref]
  7. 2016 - Demonstration of diamond-based schottky p-i-n diode with blocking voltage >500 V [Crossref]
  8. 2004 - Surface transfer doping of diamond [Crossref]
  9. 2016 - Electronic structure of hydrogenated diamond: Microscopical insight into surface conductivity [Crossref]