Electrical properties and Mott parameters of polycrystalline diamond films synthesized by HF CVD method from hydrogen/methanol gas mixture
At a Glance
Section titled “At a Glance”| Metadata | Details |
|---|---|
| Publication Date | 2017-12-20 |
| Journal | Materials Science-Poland |
| Authors | Agnieszka Banaszak-Piechowska, K. Fabisiak, E. Staryga, K. Paprocki |
| Institutions | Kazimierz Wielki University in Bydgoszcz, Lodz University of Technology |
| Citations | 2 |
| Analysis | Full AI Review Included |
Executive Summary
Section titled “Executive Summary”- Focus: Investigates the relationship between crystallographic orientation (texture) and electronic transport in Hot Filament CVD (HFCVD) polycrystalline diamond films deposited from H2/CH3OH gas mixtures.
- Methodology: Uses temperature-dependent DC conductivity (I-V-T) measurements from 90 K to 300 K to evaluate charge transport in Au/diamond/n-Si heterostructures.
- Key Finding: Conduction follows the Variable Range Hopping (VRH, Mott m = 1/4) mechanism through localized states near the Fermi level.
- Mott Parameters Extracted: Density of states N(EF) ranging from 2.21 × 1014 to 1.66 × 1015 eV-1·cm-3, hopping energy W (43.5 meV to 142.3 meV), and hopping distance R (1.49 × 10-5 cm to 2.56 × 10-5 cm).
- Correlation Demonstrated: Higher texture coefficient TC(220) correlates with higher N(EF), while decreasing crystallite size increases hopping energy W.
- Conclusion: Crystalline structure and sp2/sp3 ratio at grain boundaries directly govern electrical properties, providing a pathway to tune diamond film conductivity for electronic/sensing applications.
Technical Specifications
Section titled “Technical Specifications”| Parameter | Value | Unit | Context |
|---|---|---|---|
| Methanol Concentration | 2.3, 2.5, 2.7 | vol.% | Variable parameter for MCD-2.3, MCD-2.5, MCD-2.7 samples |
| Total Gas Flow Rate | 100 | sccm | H2/CH3OH mixture |
| Total Gas Pressure | 0.9 | Pa | Low-pressure HFCVD regime |
| Filament Temperature | 2300 | K | Measured via pyrometer |
| Substrate Temperature | 1010 | K | Measured via thermocouple |
| Growth Time | 4 | h | Per deposition run |
| Substrate | n-type Si (111) | — | Mechanically polished with 0.2 µm diamond paste |
| Crystallite Size (⟨220⟩) | 36 - 67 | nm | Calculated via XRD line broadening |
| Crystallite Size (SEM) | 300 - 1800 | nm | Surface grain dimensions |
| Preferred Orientation | ⟨220⟩ | — | Texture coefficient TC(220) = 73 % to 84 % |
| Measurement Temperature Range | 90 - 300 | K | Cryogenic to room temperature |
| Voltage Range | −5 to +5 | V | I-V characterization |
| Current Measurement | Keithley 6485 | — | Picoammeter |
| N(EF) Range | 2.21 × 1014 - 1.66 × 1015 | eV-1·cm-3 | Density of localized states at Fermi level |
| Hopping Energy (W) Range | 43.5 - 142.3 | meV | VRH activation energy |
| Hopping Distance (R) Range | 1.49 × 10-5 - 2.56 × 10-5 | cm | Average inter-site separation |
| Decay Constant (α) Range | 1.47 × 105 - 2.01 × 105 | cm-1 | Localization parameter |
| Contact Metallization | Au | — | Evaporated, nearly ohmic to diamond |
Key Methodologies
Section titled “Key Methodologies”- Substrate Preparation: n-type Si (111) wafers mechanically polished with 0.2 µm diamond paste for 10 min, ultrasonicated in nano/microdiamond/methanol suspension for 30 min, final acetone/alcohol rinse.
- Film Deposition: HFCVD system using H2/CH3OH (methanol 2.3-2.7 vol.%) at 100 sccm total flow, 0.9 Pa chamber pressure, 2300 K filament, 1010 K substrate, 4 h growth.
- Morphological Characterization: SEM (JEOL JSM-820) for grain size and surface morphology assessment.
- Structural Characterization: XRD (DRON-4, Cu-Kα radiation) for phase identification, texture coefficient calculation, and Scherrer-based crystallite size estimation.
- Device Fabrication: Au contacts thermally evaporated on diamond surface and Si backside to form Au/diamond/n-Si/Au heterostructure.
- Electrical Measurement: DC I-V-T sweeps from −5 V to +5 V at stepped temperatures from 90 K to 300 K using a Keithley 6485 picoammeter.
- Transport Modeling: Data fit to Mott Variable Range Hopping (VRH) model with m = 1/4 to extract density of states, hopping energy, and localization parameters.
6CCVD Solutions & Capabilities
Section titled “6CCVD Solutions & Capabilities”| Research Requirement | 6CCVD Offering |
|---|---|
| Polycrystalline diamond with tunable grain size & texture | Optical/Mechanical Grade PCD plates up to 125 mm, thickness 0.1 µm - 500 µm |
| High-density sp2 grain boundary engineering | Custom MPCVD-grown PCD with controlled crystallite size for tailored electronic properties |
| Ohmic Au contacts on diamond | In-house Au metalization (also Pt, Pd, Ti, W, Cu) for rapid device prototyping |
| Silicon-compatible diamond integration | PCD-on-Si via custom deposition runs, including n-type Si (111) substrates |
| Variable crystallite size (36 nm - 1.8 µm) | Engineering support for sub-100 nm nanocrystalline up to microcrystalline regimes |
| Reproducible low-pressure CVD films | MPCVD process control with tight pressure, flow, and temperature tolerances |
-
Applicable Materials: To replicate or extend this research, Polycrystalline Diamond (PCD) wafers with controlled ⟨220⟩ texture are recommended. 6CCVD’s MPCVD platform enables precise modulation of sp2/sp3 ratio at grain boundaries—the critical parameter driving VRH conduction in this study. For surface-conduction studies, our hydrogen-terminated PCD preserves the high p-type surface conductivity regimes referenced by Kawarada et al.
-
Customization Potential: The paper’s reliance on Au/diamond/n-Si/Au heterostructures is fully supported by our in-house Au evaporation capability. 6CCVD also offers custom metal stacks (Ti/Pt/Au, Ti/W, Pd) and laser cutting/patterning services for precise electrode geometry on PCD substrates up to 125 mm.
-
Engineering Support: 6CCVD’s in-house PhD team can assist with material selection for electronic transport studies, sensor platforms exploiting grain-boundary hopping conduction, and radiation-hard device development. We provide guidance on texture engineering, doping strategies (including Boron-Doped Diamond (BDD) for comparison with undoped baseline), and crystallite-size targeting to tune N(EF) and hopping parameters.
-
Call to Action: For custom specifications, prototype metallization, or material consultation on diamond-based electronic and sensing research, visit 6ccvd.com or contact our engineering team directly.
View Original Abstract
Abstract The influence of diamond crystallinity and preferred orientation on electronic conductivity of synthetic diamond films grown by hot filament chemical vapor deposition (HFCVD) was investigated. The CVD diamond films of different morphologies and crystallite sizes varying from 36 nm to 67 nm, measured in h2 2 0i direction were considered. The charge transport mechanism in the diamond samples was studied using temperature dependent DC conductivity measurements. The obtained results showed that in the temperature range of 90 K to 300 K charge transport is realized via Variable Range Hopping (VRH, m = 1/4) mechanism. Using VRH model, the Mott parameters were evaluated i.e. density of states at Fermi level N(EF) (0.22 × 1015 eV-1·cm-3 to 1.7 × 1015 eV-1·cm-3), hopping energy W (43.5 meV to 142.3 meV) and average hopping distance R (1.49 × 10-5cm to 2.56 × 10-5cm). It was shown that above mentioned parameters strongly depend on diamond film preferential orientation.